Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.22 - 1.80 g/cc | 0.0441 - 0.0650 lb/in³ | Average value: 1.47 g/cc Grade Count:259 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Density | 0.490 - 1.80 g/cc | 0.0177 - 0.0649 lb/in³ | Average value: 1.14 g/cc Grade Count:26 |
Overview of materials for Epoxy, Cast, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr.. |
|||
Density | 1.54 - 1.80 g/cc | 0.0556 - 0.0650 lb/in³ | Average value: 1.72 g/cc Grade Count:19 |
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |
|||
Density | 1.30 - 1.80 g/cc | 0.0470 - 0.0650 lb/in³ | Average value: 1.56 g/cc Grade Count:202 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Density | 1.75 - 1.80 g/cc | 0.0632 - 0.0650 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ajedium™ PVDF 9009 Polyvinylidene Fluoride (PVDF) Solef® 9009 PVDF homopolymer is a semi-crystalline fluoropolymer. Solef® film is chemically inert to most acids, aliphatic and aromatic organic compounds, chlorinated solvents and alcohols.Fea.. |
|||
Density | 1.75 - 1.80 g/cc | 0.0632 - 0.0650 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Solef® 1006 Polyvinylidene Fluoride (PVDF) Solef® 1006 PVDF is a very low viscosity homopolymer resin mainly used in injection molding or in multifilament extrusion.Features: Homopolymer; Low ViscosityUses: General PurposeAdditional Prope.. |
|||
Density | 1.75 - 1.80 g/cc | 0.0632 - 0.0650 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF) Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: MembranesAddition.. |
|||
Density | 1.75 - 1.80 g/cc | 0.0632 - 0.0650 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF) Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Features: Copolymer; Good Flexibility; Medium ViscosityAdditional Properties: Crystal.. |
|||
Density | 1.75 - 1.80 g/cc | 0.0632 - 0.0650 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF) Solef® 21510 PVDF copolymer has medium viscosity and is suitable for extrusion and for solution processing in lithium batteries applications.Features: Copolymer; Good Flexibility; Medium Viscosit.. |
|||
Density | 1.75 - 1.80 g/cc | 0.0632 - 0.0650 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF) Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional .. |
|||
Density | 1.75 - 1.80 g/cc | 0.0632 - 0.0650 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Solef® 32008 Polyvinylidene Fluoride (PVDF) Solef® 32008 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional .. |
|||
Density | 1.75 - 1.80 g/cc | 0.0632 - 0.0650 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D.. |
|||
Density | 1.75 - 1.80 g/cc | 0.0632 - 0.0650 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF) Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Features: Homopolymer; Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3417 54.0 to 6.. |
|||
Density | 1.75 - 1.80 g/cc | 0.0632 - 0.0650 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF) Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Features: High Viscosity; HomopolymerAdditional Properties: Crystallizat.. |
|||
Density | 1.75 - 1.80 g/cc | 0.0632 - 0.0650 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF) Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: Batteries; Membran.. |
|||
Density | 1.75 - 1.80 g/cc | 0.0632 - 0.0650 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF) Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Features: Copolymer; High ViscosityUses: PipingAdditional Properties: Crystallization Heat - ASTM .. |
|||
Density | 1.75 - 1.80 g/cc | 0.0632 - 0.0650 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF) Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 53... |
|||
Density | 1.30 - 1.80 g/cc | 0.0470 - 0.0650 lb/in³ | |
Goodfellow Carbon-Carbon Composite Carbon Fiber - Carbon MatrixInformation provided by Goodfellow. |
|||
Density | 1.60 - 1.80 g/cc | 0.0578 - 0.0650 lb/in³ | ISO 1138 |
Bulk Molding Compounds tetra-DUR F 4308 Bulk Molding Compound UL-licensedTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), thermal stabilit.. |
|||
Density | 1.70 - 1.80 g/cc | 0.0614 - 0.0650 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATO 159 Phenolic Molding Glass/ inorganic Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |
|||
Density | 1.77 - 1.80 g/cc | 0.0639 - 0.0650 lb/in³ | Average value: 1.79 g/cc Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), 60% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 60% Glass Reinforced". Specific grades with glass content between 55% .. |
|||
Density | 1.43 - 1.80 g/cc | 0.0517 - 0.0650 lb/in³ | Average value: 1.71 g/cc Grade Count:7 |
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass Reinforced". Each property range of values reported is.. |
|||
Density | 0.000926 - 1.80 g/cc | 0.0000335 - 0.0650 lb/in³ | Average value: 1.57 g/cc Grade Count:92 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |
|||
Density | 1.69 - 1.80 g/cc | 0.0611 - 0.0650 lb/in³ | Average value: 1.75 g/cc Grade Count:3 |
Overview of materials for Thermoset Polyurethane, Liquid, Quartz Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid, Quartz Filled". Each property range of values reported is minimum and ma.. |
|||
Density | 1.70 - 1.80 g/cc | 0.0614 - 0.0650 lb/in³ | ISO 1138 |
Bulk Molding Compounds tetra-DUR F 4306 Bulk Molding Compound Mechanical high grade standard productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion pr.. |