Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.89 g/cc | 0.0683 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 8832 C BLK This product is based on Shell's Kraton G and is used for acoustic barrier applications, exhibiting high flexibility and ease of installation. It is made exclusively for Cascade Engineering. This .. |
|||
Density | 1.89 g/cc | 0.0683 lb/in³ | |
Pyrotek TS-105 Thermoset Electrical Insulation Product (Nema Grade: G-5) Glass reinforcement, Melamine Resin, Gray color. High mechanical strength, arc and heat resistance. Self-extinguishing.ApplicationsSuperstructure support pads Bus bar insulators Pot cradle insulat.. |
|||
Density | 1.89 g/cc | 0.0683 lb/in³ | |
Pyrotek TS-109 Thermoset Electrical Insulation Product (Nema Grade: G-9) Glass reinforcement, Melamine Resin, Gray color. High mechanical strength, arc and heat resistance. Self-extinguishing.Information provided by Pyrotek. |
|||
Density | 1.89 g/cc | 0.0683 lb/in³ | |
Pyrotek TS-117 Thermoset Electrical Insulation Product (Nema Grade: GPO-1) Glass reinforcement, Polyester resin, Gray color. Economical, general purpose product.Information provided by Pyrotek. |
|||
Density | 1.89 g/cc | 0.0683 lb/in³ | |
Pyrotek TS-120 Thermoset Electrical Insulation Product (Nema Grade: GPO-2) Glass reinforcement, Polyester resin, Cream color. Highly flame resistant. Meets UL 94VO.Information provided by Pyrotek. |
|||
Density | 1.89 g/cc | 0.0683 lb/in³ | |
Pyrotek TS-207 Thermoset Electrical Insulation Product Polymer reinforcement, Polyester resin, Grey color. High strength and good electrical resistance.Information provided by Pyrotek. |
|||
Density | 1.89 g/cc | 0.0683 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Asia Pacific) Thermally conductive mineral filled PPS FR compound |
|||
Density | 1.89 g/cc | 0.0683 lb/in³ | ASTM D792A |
Resinoid 1382 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Density | 1.89 g/cc | 0.0683 lb/in³ | |
Pyrotek Pyrocast ICL Castable Refractory Pyrocast ICL was developed exclusively for the induction furnace market as a coil lining refractory. This silica and alumina based material displays high strength and excellent thermal shock resist.. |
|||
Density | 1.89 g/cc | 0.0683 lb/in³ | ASTM D572 |
Haysite 14100 Polyester BMC, 15% Glass Reinforced The 14100 series bulk molding compound is an electrical grade material that can be compression, transfer, or injection molded. Offering good mechanical strength and excellent electrical properties, .. |
|||
Density | 1.89 g/cc | 0.0683 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® LC200 PFPE Lubricant FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir.. |
|||
Density | 1.89 g/cc | 0.0683 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® W500 PFPE Lubricant Fomblin® PFPE fluorinated lubricants are used when harsh chemical environments, high temperatures or wide working-temperature ranges are encountered.Information provided by Solvay Solexis, Inc. |
|||
Density | 1.89 g/cc | 0.0683 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® Y L-VAC 14/6 PFPE Pump Oil FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and.. |
|||
Density | 1.89 g/cc | 0.0683 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® Y L-VAC 16/6 PFPE Pump Oil FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and.. |
|||
Density | 1.89 g/cc | 0.0683 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp 5X06476 FP-V (PVDF) LNP* FP-VM-3830 is a compound based on Polyvinylidine Fluoride (PVDF) containing Mineral.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.89 g/cc | 0.0683 lb/in³ | |
Saint-Gobain Rulon® F Grade Bearing/Seal PTFE F Grade Bearing/Seal PTFE is used for applications requiring a long wearing material, especially in dry applications and those requiring high abrasion resistance. Standard tape liner material for Ru.. |
|||
Density | 1.89 g/cc | 0.0683 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America SI 9550 Silicone Compound SI 9550 is a short fiberglass reinforced silicone molding compound, which offers moderate strength properties, and dimensional stability and excellent long-term thermal stability at elevated tempera.. |
|||
Density | 1.89 g/cc | 0.0683 lb/in³ | ASTM D792 |
Plenco 1501 Polyester, Briquette, Compression Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Density | 1.89 g/cc | 0.0683 lb/in³ | ASTM D792 |
Plenco 1501 Polyester, Briquette, Transfer Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Density | 1.89 g/cc | 0.0683 lb/in³ | ASTM D792 |
Plenco 1586 Polyester, Pellet, Injection Molded PLENCO 01586 is a glass and mineral reinforced pelletized polyester molding compound offering excellent heat resistance and mechanical strength properties. This product is typically used for injecti.. |
|||
Density | 1.89 g/cc | 0.0683 lb/in³ | |
3M Dyneon™ Fluorel™ FLS-2650 Fluoroelastomer VF2 + HFP + TFE Terpolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 70.3%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 1.8% Luperco™ 101XL Peroxide, and 2.5 % Triallyl .. |