Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 1.91 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.91 g/cc
0.0690 lb/in³
ISO 1183
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Europe-Africa-Middle East)
Thermally conductive mineral and glass fiber filled PPS Eco-FR compound
Density 1.91 g/cc
0.0690 lb/in³
50% Resin Content; Internal Method
Park Electrochemical Nelco® N4000-13 High-Speed Multifunctional Epoxy Laminate and Prepreg
The Nelco® N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. N4000-13 SI® is excellent for applic..
Density 1.91 g/cc
0.0690 lb/in³
Cookson Group Plaskon® SMT-B-1F Epoxy Molding Compound for PBGAs  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for PBGA applications. It has the same unique resin system as SMT-B-1, which mi..
Density 1.91 g/cc
0.0690 lb/in³
Cookson Group Plaskon® SMT-B-1FX (146.801) Epoxy Molding Compound for PBGAs  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for PBGA applications. It is a reduced catalyst version of SMT-B-1F and provide..
Density 1.91 g/cc
0.0690 lb/in³
Industrial Laminates/Norplex MC511A Glass Fabric
Description: MC511A is a high strength, glass epoxy laminate that is specially formulated to meet power generation producer's exacting standards where higher strength at elevated temperatures ar..
Density 1.91 g/cc
0.0690 lb/in³
LATI Laticonther 62 CPG/500 PA 6, Glass Fiber Reinforced
High thermal conductivity product based on Polyamide 6 (PA6). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..
Density 1.91 g/cc
0.0690 lb/in³
LATI Laticonther 80 GCE/650 PPS, Glass/Mineral Reinforced
High thermal conductivity product based on Polyphenylene Sulfide (PPS). Glass fibers / Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformatio..
Density 1.91 g/cc
0.0690 lb/in³
ASTM D891
Solvay Specialty Polymers FOMBLIN® Y H-VAC 40/11 PFPE Pump Oil
FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and..
Density 1.91 g/cc
0.0690 lb/in³
ASTM D891
Solvay Specialty Polymers FOMBLIN® Y45 PFPE Lubricant
FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporati..
Density 1.91 g/cc
0.0690 lb/in³
ASTM D891
Solvay Specialty Polymers FOMBLIN® YPL1500 PFPE Lubricant
FOMBLIN YR perfluoropolyether fluids have excellent high temperature stability, good low temperature properties, very good E.P. and wear characteristics, good evaporative loss, and good viscosity in..
Density 1.91 g/cc
0.0690 lb/in³
ASTM D891
Solvay Specialty Polymers FOMBLIN® YR PFPE Lubricant
FOMBLIN YR perfluoropolyether fluids have excellent high temperature stability, good low temperature properties, very good E.P. and wear characteristics, good evaporative loss, and good viscosity in..
Density 1.91 g/cc
0.0690 lb/in³
ASTM D792
Sumitomo Bakelite North America 52-70-70-VO-P Short-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Conforms with the requirements of ASTM D5948 Type..
Density 1.91 g/cc
0.0690 lb/in³
ASTM D792
Sumitomo Bakelite North America 73-70-70 C-P /73-70-70 VO-P Short-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I..
Density 1.91 g/cc
0.0690 lb/in³
ASTM D792
Sumitomo Bakelite North America RX® 2-520 Short-Glass Reinforced Diallyl Phthalate
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SI..
Density 1.91 g/cc
0.0690 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP 2F006 ETFE
LNP* THERMOCOMP* 2F006 is a compound based on ETFE containing 30% Glass Fiber.
Density 1.91 g/cc
0.0690 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Thermocomp MH0200A PP (Europe-Africa-Middle East)
LNP* Thermocomp* MH0200A is a compound based on Polypropylene resin containing High Specific Gravity Filler.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Density 1.91 g/cc
0.0690 lb/in³
ASTM D792
Toyobo VYLOPET® EMC130-20 Injection Molding Polyester Resin, Flame Resistant
Applications: Relay partsFeatures: Excellent arc resistanceFlame resistanceInformation provided by Toyobo.
Density 1.91 g/cc
0.0690 lb/in³
ASTM D792
Dow Fulcrum™ Thermoplastic Glass-Filled Polyurethane Composite Strip
FULCRUM Thermoplastic Composite Technology is specifically designed for the fabrication of continuous fiber composites that have greater flexibility in post-processing operations as well as higher t..
Density 1.91 g/cc
0.0690 lb/in³
ISO 1183
Eurostar Starpylen HU 70E3 HDPE, Injection Molding
Starpylen HU 70E3 is a High Density Polypropylene Injection Molding Resin (also known as HU70E3)Information provided by Eurostar.
Density 1.91 g/cc
0.0690 lb/in³
ISO 1183
Eurostar Starpylen MH0200A HDPE, Injection Molding
Starpylen MH0200A is a High Density Polypropylene Injection Molding ResinInformation provided by Eurostar.
Density 1.91 g/cc
0.0690 lb/in³
ISO 1183
LATI LARTON CE/60 60% Special Mineral Filled Polyphenylene sulfide (PPS)  (Unverified Data**)
Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex..
Density 1.91 g/cc
0.0690 lb/in³
Relative Density; ASTM D792
Sumitomo Bakelite North America FS-10-VO-200-P Short-Glass Reinforced Diallyl Phthalate
Short glass fiber reinforced, flame retardant, diallyl meta-phthalate molding compound with excellent heat resistance.Meets the requirements of ASTM D5948 Type SIG-F.Information provided by Vyncolit..
Density 1.91 g/cc
0.0690 lb/in³
Relative Density; ASTM D792
Sumitomo Bakelite North America FS-5 Short-Glass Reinforced Diallyl Phthalate
Short glass fiber reinforced, non-flame retardant, diallyl meta-phthalate molding compound which meets the requirements of ASTM D5948 TYPE SIG.Information provided by Vyncolit, a Sumitomo Bak Group
Copyright © lookpolymers.com All Rights Reserved