Physical Properties Metric English Comments
Density 2.00 - 2.10 g/cc
0.0723 - 0.0759 lb/in³
ASTM D792
Polikim EFALON® K-35 PTFE, 35% Carbon Filled
K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings...
Density 0.000657 - 2.10 g/cc
0.0000237 - 0.0759 lb/in³
Average value: 1.16 g/cc Grade Count:154
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..
Density 1.64 - 2.10 g/cc
0.0592 - 0.0759 lb/in³
Average value: 1.85 g/cc Grade Count:35
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor..
Density 1.55 - 2.10 g/cc
0.0560 - 0.0759 lb/in³
Average value: 1.87 g/cc Grade Count:23
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum ..
Density 2.04 - 2.10 g/cc
0.0737 - 0.0759 lb/in³
extruded; ASTM D792
Guarniflon PTFE G453 Polytetrafluoroethylene 25% Carbographite
PTFE G Standard Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high ..
Density 2.04 - 2.10 g/cc
0.0737 - 0.0759 lb/in³
extruded; ASTM D792
Guarniflon PTFE G415 Polytetrafluoroethylene 25% Soft Carbon
PTFE G Standard Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high ..
Density 1.85 - 2.10 g/cc
0.0668 - 0.0759 lb/in³
Molding; IS 867-1963
Amity Thermosets ATR 457© Phenolic Molding Glass fiber Filler, Compression Molded
Characteristics:High shock resistant ( high impact strength ) High Mechanical StrengthHigh Dielectric StrengthHigh Electrical Insulation Color- pale brown Medium flow Applications:Electric motor en..
Density 1.90 - 2.10 g/cc
0.0686 - 0.0759 lb/in³
Molded
Bulk Molding Compounds BMC T12-15526 General Purpose Molding Compound
BMC T12-15526 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. ..
Density 1.90 - 2.10 g/cc
0.0686 - 0.0759 lb/in³
ISO 1138
Bulk Molding Compounds tetra-DUR N 4203 Bulk Molding Compound
Highest dimensional stability under temp. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipat..