Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.30 g/cc | 0.0831 lb/in³ | Green |
Nabaltec NABALOX® NO 713-10 MF Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 2.30 g/cc @Temperature 20.0 °C |
0.0831 lb/in³ @Temperature 68.0 °F |
liquid |
Oceanchem Group Zinc Bromide Molecular Formula: ZnBr2Cas No.: 7699-45-8Mainly applied in ocean oil wells as complete liquid, stationary liquid and amend liquid.Information Provided by Oceanchem Group |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | ISO 1183-1 |
Quadrant EPP Fluorosint® 207 PTFE + mica, compression moulded (ISO Data) This material has a food contact compliant composition which, in combination with the good mechanical performance, dimensional stability, sliding and wear properties and inherent outstanding chemica.. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | ISO 1183-1 |
Quadrant EPP Semitron® ESd 500HR PTFE, static dissipative, extruded (ISO Data) Reinforced with a proprietary synthetic mica, Semitron ESd 500HR offers an excellent combination of low frictional properties, good dimensional stability and electrostatic dissipation. Whenever virg.. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | |
MarkeTech Repton EXP 48 Cordierite Mg-Al-Si Oxide REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | 2.3 g/cc Average. Minimum bulk density is 2.277 g/cc. |
Materion E40 Beryllium/BeO Composite, 40 Volume% BeO Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop.. |
|||
Density | 2.30 - 3.00 g/cc | 0.0831 - 0.108 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 586.1 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr) |
|||
Density | 2.30 - 3.00 g/cc | 0.0831 - 0.108 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 599.063 Agglomerated Sintered Molybdenum Carbide (Cr2O3) |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP AH0230A ABS LNP THERMOCOMP* AH0230A is a compound based on ABS resin. Added feature of this material is: High Specific Gravity. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP AH0230A ABS LNP THERMOCOMP* AH0230A is a compound based on ABS resin. Added feature of this material is: High Specific Gravity. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP AH0230A ABS (Asia Pacific) LNP THERMOCOMP* AH0230A is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: High Specific Gravity. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP AH0230A ABS (Europe-Africa-Middle East) LNP THERMOCOMP* AH0230A is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: High Specific Gravity. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | ASTM D792 |
Techmer ES HiFill® ABS HI 0230 High Impact Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Density and High Impact ResistanceProcessing Method: Injection MoldingInformation provided by .. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | |
Trelleborg Emerson & Cuming Stycast® 906-1 One-Component Epoxy High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | |
Dandong Taico Minerals TAICOCITE® TC35 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | |
Dandong Taico Minerals TAICOCITE® TC50 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | |
Dandong Taico Minerals TAICOCITE® TC8 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | |
Dandong Taico Minerals TAICOCITE® TC3 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | |
Dandong Taico Minerals TAICOCITE® TC80 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | |
COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | |
Accuratus Accuflect™ Light-Reflecting Ceramic Accuflect™ is a specially formulated and processed ceramic developed by Accuratus to satisfy the market demand for diffuse reflectors in high temperature and high energy environments.Key Property: .. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | |
Arlon AD255A Glass, PTFE and Micro-Dispersed Ceramic Lower Loss and Improved Performance over Traditional AD Series.Information provided by Arlon Materials for Electronics (MED). |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | ASTM D792 Method A |
Arlon AD255C PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs For RF & Microwave Printed Circuit Boards. Very Low Loss PTFE and Ceramic Filled Composite (0.0014 Loss Tangent at 10GHz and Base Station Frequencies)Dielectric Constant (2.55) with Tighter Toleran.. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | |
BASF Paliotan® Yellow L 1240 Color Additive Description: Economical lead free pigment with good hiding, high chroma and color strengthSuitable for: Baking systems |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | |
Anderman Ceramics EM60P Sillimanite Porous synthetic mullite with high thermal shock. Available as tube up to 10 ft (3 m) long with diameters 0.6" to 2.4".Information provided by Anderman Ceramics. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | |
CeramTec 547 Cordierite (2MgO-2Al2O3-5SiO2) Te value is 670°C. Hasselman Thermal Shock value is 800 K.Data provided by CeramTec North America. |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | ISO 1183 |
Barlog Plastics KEBABLEND W/H 23.10.1 PBT functional compound, high density PBT mod.Information provided by BARLOG plastics GmbH. |
|||
Density | 2.30 - 3.00 g/cc | 0.0831 - 0.108 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 588.088 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) 53/20 µm |
|||
Density | 2.30 g/cc | 0.0831 lb/in³ | Apparent |
Gouda Vuurvast AK 45 Dense Refractory Brick Description: High quality refractory brick with a good volume stability up to 1450°C. Used where high load bearing capacities are required e.g. blast furnace stoves.Remarks: This data represents av.. |