Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 6.92 g/cc | 0.250 lb/in³ | |
Lucas-Milhaupt AL 802 Aluminum Brazing Filler Metal Characteristics:AL 802 is a general purpose free flowing soldering filler metals for use with all solderable aluminum and aluminum alloys when soldering with torch. Information provided by Lucas-Mi.. |