Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
Pacific Sintered Materials F-240-S(HT) Steel Powdered Metal Applications:Medium stressed mechanical componentsEquivalent MPIF Specification: F-0005-60(HT)All information provided by Pacific Sintered Metals. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
Pacific Sintered Materials F-241-S Iron Powdered Metal Applications:Low stressed mechanical componentsSoft magnetic applicationsEquivalent MPIF Specification: F-0000-15All information provided by Pacific Sintered Metals. |
|||
Density | 7.00 - 7.20 g/cc | 0.253 - 0.260 lb/in³ | |
Pacific Sintered Materials F-241-S2 Iron Soft Magnetic Powdered Metal Applications: DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores.Equivalent ASTM Specification: B310-70, TYPE IV, CLASS AAll information provided by Pa.. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
Pacific Sintered Materials F-244-S High Carbon Steel Powdered Metal Applications:Highly stressed mechanical componentsGood hardenabilityEquivalent MPIF Specification: F-0008-35All information provided by Pacific Sintered Metals. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
Pacific Sintered Materials F-244-S(HT) High Carbon Steel Powdered Metal Applications:Highly stressed mechanical componentsGood hardenabilityEquivalent MPIF Specification: F-0008-85(HT)All information provided by Pacific Sintered Metals. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
Pacific Sintered Materials FCC-214-S High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
Pacific Sintered Materials FCC-214-S(HT) High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
Pacific Sintered Materials FN-250-S Nickel Iron Powdered Metal Good impact resistant mechanical components. Good hardenability.Equivalent MPIF Specification: FN-0200-20All information provided by Pacific Sintered Metals. |
|||
Density | 7.00 - 7.20 g/cc | 0.253 - 0.260 lb/in³ | |
Pacific Sintered Materials FN-251-S Invar Powdered Metal Coefficient of thermal expansion equal to glass.All information provided by Pacific Sintered Metals. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
Pacific Sintered Materials FN-253-S(HT) 4600 Powdered Metal High performance material with high strength and wear resistance after heat treatment.Equivalent MPIF Specification: FL-4605-100HTAll information provided by Pacific Sintered Metals. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
Pacific Sintered Materials FN-262-S High Strength Nickel Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability.Equivalent MPIF Specification: FN-0405-35All information provided by Pacific Sintered Metals. |
|||
Density | 7.00 - 7.20 g/cc | 0.253 - 0.260 lb/in³ | |
Pacific Sintered Materials FP-1650-S Phosphorous Iron Soft Magnetic Powdered Metal For applications requiring high yield strength and toughness. Magnetic properties superior to iron, but slightly inferior to silicon iron.All information provided by Pacific Sintered Metals. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals 4600 FN-253-S(HT) Powdered Metal High performance material with high strength and wear resistance after heat treatment Equivalent MPIF Specification: FL-4605-100HTInformation Provided by Pacific Sintered Metals, a division of PSM .. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-214-S Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP.. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals High Carbon Steel F-244-S Powdered Metal Highly stressed mechanical components, Good hardenability Equivalent MPIF Specification: F-0008-35Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals High Carbon Steel F-244-S(HT) Powdered Metal Highly stressed mechanical components, Good hardenability Equivalent MPIF Specification: F-0008-85(HT)Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 7.00 - 7.20 g/cc | 0.253 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals Iron Nickel FN-252-S Powdered Metal Very low coercive force and high permeability. Excellent for shielding and switching applications.Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals Nickel Steel FN-255-S Powdered Metal Good impact resistant mechanical components, Good hardenability Equivalent MPIF Specification: FN-0205-25Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 7.00 - 7.20 g/cc | 0.253 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals Phosphorous Iron FP-1650-S Powdered Metal For applications requiring high yield strength and toughness. Magnetic properties superior to iron, but slightly inferior to silicon iron.Information Provided by Pacific Sintered Metals, a division .. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals Steel F-240-S Powdered Metal Medium stressed mechanical components Equivalent MPIF Specification: F-0005-25Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals Steel F-240-S(HT) Powdered Metal Medium stressed mechanical components Equivalent MPIF Specification: F-0005-60(HT)Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals Nickel Iron FN-250-S Powdered Metal Good impact resistant mechanical components, Good hardenability Equivalent MPIF Specification: FN-0200-20Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals Nickel Steel FN-255-S(HT) Powdered Metal Good impact resistant mechanical components, Good hardenability Equivalent MPIF Specification: FN-0208-130HTInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 6.64 - 7.20 g/cc | 0.240 - 0.260 lb/in³ | Approximately 10% lighter than carbon steel |
Dura-Bar 100-70-03 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
Density | 6.64 - 7.20 g/cc | 0.240 - 0.260 lb/in³ | Approximately 10% lighter than carbon steel |
Dura-Bar 120-90-02 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
Density | 6.64 - 7.20 g/cc | 0.240 - 0.260 lb/in³ | Approximately 10% lighter than carbon steel |
Dura-Bar 60-40-18 Continuously Cast Ductile Iron Bar Stock ASTM A536, 4018 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
Density | 6.64 - 7.20 g/cc | 0.240 - 0.260 lb/in³ | Approximately 10% lighter than carbon steel |
Dura-Bar 65-45-12 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-214-S(HT) Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP.. |
|||
Density | 7.00 - 7.20 g/cc | 0.253 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals Invar FN-251-S Powdered Metal Coefficient of thermal expansion equal to glassInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 7.00 - 7.20 g/cc | 0.253 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals Iron F-241-S2 Powdered Metal DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores Equivalent ASTM Spec: B310-70, Type IV, Class AInformation Provided by Pacific Sintered Metals, a d.. |