Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.60 - 9.80 g/cc | 0.347 - 0.354 lb/in³ | |
MarkeTech Cu/Mo/Cu 1:3:1 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |
|||
Density | 9.60 - 9.80 g/cc | 0.347 - 0.354 lb/in³ | |
MarkeTech Mo70Cu Moly/Copper Heat Sink Material MoCu alloys are made by sintering molybdenum and copper together. This results in a heat sink of lower density than tungsten-based materials, low thermal expansion, and excellent thermal conductivit.. |