Physical Properties | Metric | English | Comments |
---|---|---|---|
Nitrogen Transmission | 20.0 - 104 cc-mm/m²-24hr-atm | 50.8 - 263 cc-mil/100 in²-24hr-atm | Average value: 32.0 cc-mm/m²-24hr-atm Grade Count:14 |
Overview of materials for Modified ETFE, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Modified ETFE, Unreinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Nitrogen Transmission | 20.0 cc-mm/m²-24hr-atm | 50.8 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON EA-LR43 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Nitrogen Transmission | 20.0 cc-mm/m²-24hr-atm | 50.8 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON EC-6500 ETFE Coating Powder, White Description: 0.3-1.0 mm thickness.Processing Methods:Electro-static spray coating.Information provided by Daikin Industries. |
|||
Nitrogen Transmission | 20.0 cc-mm/m²-24hr-atm | 50.8 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON EC-6520 ETFE Coating Powder, White Description: 0.1-0.3 mm thickness.Processing Methods:Electro-static spray coating.Information provided by Daikin Industries. |
|||
Nitrogen Transmission | 20.0 cc-mm/m²-24hr-atm | 50.8 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON EP-610 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Nitrogen Transmission | 20.0 cc-mm/m²-24hr-atm | 50.8 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON EP-610AS ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Nitrogen Transmission | 20.0 cc-mm/m²-24hr-atm | 50.8 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON EPW-1605GN ETFE Liquid Primer, Green Description: 10-60 micron thickness.Processing Methods:Air spray coating.Information provided by Daikin Industries. |
|||
Nitrogen Transmission | 20.0 cc-mm/m²-24hr-atm | 50.8 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON EPW-1606BL ETFE Liquid Primer, Blue Description: 10-60 micron thickness.Processing Methods:Air spray coating.Information provided by Daikin Industries. |
|||
Nitrogen Transmission | 20.0 cc-mm/m²-24hr-atm | 50.8 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON RP-4020 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Nitrogen Transmission | 20.0 cc-mm/m²-24hr-atm | 50.8 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON RP-4040 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Nitrogen Transmission | 20.0 cc-mm/m²-24hr-atm | 50.8 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON RP-5000 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Nitrogen Transmission | 20.0 cc-mm/m²-24hr-atm | 50.8 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON RP-5000AS EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Nitrogen Transmission | 20.0 cc-mm/m²-24hr-atm | 50.8 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON EC-6820 ETFE Coating Powder, White Description: 0.5-5.0 mm thickness.Processing Methods:Roto lining.Information provided by Daikin Industries. |
|||
Nitrogen Transmission | 20.0 cc-mm/m²-24hr-atm | 50.8 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON EP-620 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Nitrogen Transmission | 20.0 cc-mm/m²-24hr-atm | 50.8 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON EC-6510 ETFE Coating Powder, White Description: 0.3-2.0 mm thickness.Processing Methods:Electro-static spray coating.Information provided by Daikin Industries. |
|||
Nitrogen Transmission | 20.0 cc-mm/m²-24hr-atm | 50.8 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON EPW-1609BK ETFE Liquid Primer, Black Description: 10-60 micron thickness.Processing Methods:Air spray coating.Information provided by Daikin Industries. |