Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0124 cm/cm

@Time 86400 sec
0.0124 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP KX97390 Acetal Copolymer
LNP THERMOCOMP* KX97390 is a compound based on Acetal Copolymer resin containing Glass Fiber. Added features of this material include: Chemically Coupled.
Linear Mold Shrinkage, Transverse 0.0124 cm/cm

@Time 86400 sec
0.0124 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP RF004 PA 66
LNP THERMOCOMP* RF004 is a compound based on Nylon 66 resin containing 20% Glass Fiber.
Linear Mold Shrinkage, Transverse 0.0124 cm/cm

@Time 86400 sec
0.0124 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP RF004XXD PA 66
LNP THERMOCOMP* RF004XXD is a compound based on Nylon 66 resin containing 20% Glass Fiber.