Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0146 cm/cm @Time 86400 sec |
0.0146 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Europe-Africa-Middle East) LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0146 cm/cm @Time 86400 sec |
0.0146 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 LNP* KONDUIT* RTF2B is a compound based on Nylon 66 resin containing 10% Glass Fiber, 55% Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0146 cm/cm @Time 86400 sec |
0.0146 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Asia Pacific) LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |