Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.190 g/cc | 0.00686 lb/in³ | ASTM D1895 |
Kraton® G1640 E (SEBS) Linear Triblock Copolymer Description: Kraton G1640 E is a clear linear triblock copolymer based on styrene and ethylene/butylene (S-E/B-S) with bound styrene of 32.9% mass. It is supplied from Europe as identified in the gr.. |
|||
Bulk Density | 0.190 g/cc | 0.00686 lb/in³ | EN ISO 60 |
Gwent Electronic Materials P2121112P11 Oxygen Plasma Modified Multiwalled Carbon Nanotubes Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Bulk Density | 0.190 g/cc | 0.00686 lb/in³ | EN ISO 60 |
Gwent Electronic Materials P2121112P12 Acid Vapor Plasma Modified Single and Double Walled Carbon Nanotubes Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Bulk Density | 0.190 g/cc | 0.00686 lb/in³ | EN ISO 60 |
Gwent Electronic Materials P2121112P13 Argon Plasma Modified Single and Double Walled Carbon Nanotubes Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Bulk Density | 0.190 g/cc | 0.00686 lb/in³ | EN ISO 60 |
Gwent Electronic Materials P2121112P14 Nitrogen Plasma Modified Single and Double Walled Carbon Nanotubes Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Bulk Density | 0.190 g/cc | 0.00686 lb/in³ | EN ISO 60 |
Gwent Electronic Materials P2121112P15 Ammonia Plasma Modified Single and Double Walled Carbon Nanotubes Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Bulk Density | 0.190 g/cc | 0.00686 lb/in³ | EN ISO 60 |
Gwent Electronic Materials P2121112P16 Oxygen Plasma Modified Single and Double Walled Carbon Nanotubes Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Bulk Density | 0.190 g/cc | 0.00686 lb/in³ | EN ISO 60 |
Gwent Electronic Materials P2121112P18 Nitrogen Plasma Modified Multiwalled Carbon Nanotubes Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Bulk Density | 0.190 g/cc | 0.00686 lb/in³ | EN ISO 60 |
Gwent Electronic Materials P2121112P19 Tetrafluoromethane Plasma modified Single and Double Walled Carbon Nanotubes Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Bulk Density | 0.190 g/cc | 0.00686 lb/in³ | EN ISO 60 |
Gwent Electronic Materials P2121112P7 Acid Vapor Plasma Modified Multiwalled Carbon Nanotubes Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Bulk Density | 0.190 g/cc | 0.00686 lb/in³ | EN ISO 60 |
Gwent Electronic Materials P2121112P8 Argon Plasma Modified Multiwalled Carbon Nanotubes Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Bulk Density | 0.190 g/cc | 0.00686 lb/in³ | EN ISO 60 |
Gwent Electronic Materials P2121112P9 Tetrafluoromethane Plasma Modified Multiwalled Carbon Nanotubes Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Bulk Density | 0.190 g/cc | 0.00686 lb/in³ | EN ISO 60 |
Gwent Electronic Materials P2121112P10 Ammonia Plasma Modified Multiwalled Carbon Nanotubes Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Bulk Density | 0.190 g/cc | 0.00686 lb/in³ | Scott |
TIMCAL TIMREX® KC44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Bulk Density | 0.190 g/cc | 0.00686 lb/in³ | Scott, Typical |
TIMCAL TIMREX® KS44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Bulk Density | 0.190 g/cc | 0.00686 lb/in³ | Scott |
TIMCAL TIMREX® SFG44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Bulk Density | 0.190 g/cc | 0.00686 lb/in³ | Scott, Typical |
TIMCAL TIMREX® C-LUB 310 Primary Synthetic Graphite Information provided by TIMCAL |
|||
Bulk Density | 0.190 - 0.260 g/cc | 0.00686 - 0.00939 lb/in³ | |
Zircar Ceramics ASQ Castertip 14 pcf density refractory ceramic fiber "soft tip". Alumina bonding of shot free fiber results in extreme performance in manufacture of the finest grades of medical, food and packaging foils. Inform.. |