Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | |
Zircar Zirconia HfF-100 Hafnia Felt Insulation Our hafnia (HfO2) fibers and textiles are made by the same unique Zircar process used for manufacturing yttria-stabilized zirconia cloths and felts. Our high purity hafnia fiber and textiles are off.. |
|||
Bulk Density | <= 0.500 g/cc | <= 0.0181 lb/in³ | |
Magyar Aluminum ALOLT 50AF Aluminum Hydroxide Ground type |
|||
Bulk Density | 0.500 - 0.580 g/cc | 0.0181 - 0.0210 lb/in³ | ASTM D1895 |
LG Chemical LS100 PVC General Description: LS100 is a general-purpose product used for soft and hard products and is most widely used in PVC grade.Main Applications: Pipe, power cable jacket, leather, sheets, hoses, soft.. |
|||
Bulk Density | 0.500 - 1.20 g/cc | 0.0181 - 0.0434 lb/in³ | Apparent Density |
Indium Corp. Fine ITO Indium Tin Oxide Indium Tin Oxide (ITO, or tin-doped indium oxide) is a mixture of indium(III) oxide and tin(IV) oxide, typically 90% indium oxide, 10% tin oxide by weight. In powder form it is yellow-green in colo.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
Shandong Dongyue Polymer DF-21A PTFE Presintered Resin Usage: The presintered resin is suitable for continuously extruding of all types, pushing and pressing PTFE rod, tube and special shape.Packing: PTFE is packed in double layer PVC bags inside and in.. |
|||
Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America RX® 525 Cellulose Reinforced Phenolic Novolac RX 525 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for parts requiring moderate toughness. It is designed to meet the requirements of ASTM D-594.. |
|||
Bulk Density | 0.500 - 0.600 g/cc | 0.0181 - 0.0217 lb/in³ | |
Borealis Borseal™ RE239CF Polypropylene Copolymer Borseal™ RE239CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films for metallization. Applications: Borseal™ RE239CF is recommended for food packaging, high.. |
|||
Bulk Density | 0.500 - 0.600 g/cc | 0.0181 - 0.0217 lb/in³ | |
Borealis SuperCOPO™ LH4201R Polyethylene Insulation Compound, Crosslinkable SuperCOPO™ LH4201R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications: SuperCOPO™ LH4201R is intended for insulation of XLPE power cabl.. |
|||
Bulk Density | 0.500 - 0.650 g/cc | 0.0181 - 0.0235 lb/in³ | |
Addcomp ADD-VANCE® FR 495 PP copolymer based flame-retardant compound Fields of application: Injection moulded, or moulded articles (> 1,5 mm thickness) produced via Direct LFT processesExamples: Moulding parts such a under body panels, door modules, industrial parts,.. |
|||
Bulk Density | 0.500 - 0.600 g/cc | 0.0181 - 0.0217 lb/in³ | |
Addcomp ADD-VANCE® UV 442 PP based anti-UV masterbatch Fields of application: Foils, films, fibres, extruded and injection moulded articles made from PE and PP compatible resins, like PP, PP/EDPM, PP/PE/EDPM blends (TPOs).Examples: Automotive bumpers, a.. |
|||
Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | ASTM D1895 |
ALM PA 850 Black Nylon 11 SLS Prototyping Polymer Information provided by Advanced Laser Materials (ALM). |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Dry) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Dry) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® KR 4355 G5 BK 00564 25% Glass Filled PA6/6T (Conditioned) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® A3HG6 HR BK 23591 30% Glass Filled PA66 (Dry) Description: 30% glass-fiber reinforced injection-molding grade with enhanced hydrolysis resistance, e.g., for applications in vehicle cooling systems.Information provided by BASF |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® A3XZG5 BK 23187 25% Glass Filled PA66 FR (Conditioned) Description: Impact-modified, 25% glass-fiber reinforced injection-molding grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; for compone.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B35G3 BK 00564 15% Glass Filled PA6 (Conditioned) Description: 15% glass fiber reinforced injection molding grade e.g. for internal gas pressure applications such as flashing direction switch gears, automobile mirror housings and wheels of mountain.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Conditioned) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Bulk Density | 0.500 - 0.650 g/cc | 0.0181 - 0.0235 lb/in³ | |
Addcomp ADD-VANCE® NU 559 Nucleation masterbatch, PP based Fields of application: Extruded and injection molded articles made from PP and PE resins.Examples: Extruded sheets, films, tapes and blow molded, compression molded and injection molded articles, su.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® A3HG5 LS BK 23189 25% Glass Filled PA66 (Dry) Description: 25% glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used fo.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3M6 Grey 22319 Q94 30% Mineral Filled PA6 (Dry) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3UG4 LS BK 23215 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3WG6 GP BK 23210 30% Glass Filled PA6 (Conditioned) Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade used e.g. for automobile manifold.Information provided by BASF |
|||
Bulk Density | 0.500 - 0.650 g/cc | 0.0181 - 0.0235 lb/in³ | |
Addcomp ADD-VANCE® FR 243 Halogen-free flame retardant masterbatch, PP based Fields of application: Foils, films, fibers and extruded articles made from PP with a high surface/volume ratio.Examples: Foils, films, tapes, ropes, and filaments / fibers for carpets, non-wovens, .. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3WG5 BK 00564 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |