Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.670 g/cc | 0.0242 lb/in³ | |
Zircar Zirconia CeW-15 Ceria Woven Textile Insulation Ceria (cerium dioxide), CeO2, has a very high surface area and is ideal as a catalyst support. Our ceria fibers and textiles are made by the same unique Zircar process used for manufacturing yttria-.. |
|||
Bulk Density | 0.670 g/cc | 0.0242 lb/in³ | |
Zircar Zirconia CeW-30 Ceria Woven Textile Insulation Ceria (cerium dioxide), CeO2, has a very high surface area and is ideal as a catalyst support. Our ceria fibers and textiles are made by the same unique Zircar process used for manufacturing yttria-.. |
|||
Bulk Density | 0.670 g/cc | 0.0242 lb/in³ | |
Struktol ZINC STEARATE CM A clear melt zinc stearate, is manufactured from high quality stearic acid in a tightly controlled production operation that guarantees product uniformity.STRUKTOL® Zinc Stearate CM, a clear melt.. |
|||
Bulk Density | 0.670 g/cc | 0.0242 lb/in³ | ASTM D1895 |
Plenco 00732 Melamine-Phenolic, Granular, Compression Molded PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 007.. |
|||
Bulk Density | 0.670 g/cc | 0.0242 lb/in³ | ASTM D1895 |
Plenco 00732 Melamine-Phenolic, Granular, Injection Molded PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 007.. |
|||
Bulk Density | 0.670 g/cc | 0.0242 lb/in³ | ASTM D1895 |
Plenco 3509 Phenolic, Granular, Injection Molded PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file.. |
|||
Bulk Density | 0.670 g/cc | 0.0242 lb/in³ | ASTM D1895 |
Plenco 6582 Phenolic, Briquette, Injection Molded PLENCO 06582 is a rubber modified phenolic molding compound, offering excellent heat resistant properties, along with improved mechanical strength at elevated temperatures. UL recognized under compo.. |
|||
Bulk Density | 0.670 g/cc | 0.0242 lb/in³ | Scott |
TIMCAL TIMREX® KS150-600SP Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Bulk Density | 0.670 g/cc | 0.0242 lb/in³ | ISO 60 |
Vyncolit X7255 Glass Fiber Reinforced Novolac Phenolic Novolac resin based, glass fiber and glass beads reinforced. Very easy to transform in complex shapes. Excellent mechanical and thermal properties. Higher isotropic properties and good dimensional s.. |
|||
Bulk Density | 0.670 g/cc | 0.0242 lb/in³ | |
Zircar Zirconia CeW-15 Ceria Woven Textile Insulation Ceria (cerium dioxide), CeO2, has a very high surface area and is ideal as a catalyst support. Our ceria fibers and textiles are made by the same unique Zircar process used for manufacturing yttria-.. |
|||
Bulk Density | 0.670 g/cc | 0.0242 lb/in³ | |
Zircar Zirconia CeW-30 Ceria Woven Textile Insulation Ceria (cerium dioxide), CeO2, has a very high surface area and is ideal as a catalyst support. Our ceria fibers and textiles are made by the same unique Zircar process used for manufacturing yttria-.. |
|||
Bulk Density | 0.670 g/cc | 0.0242 lb/in³ | ASTM D1895 |
Plenco 4304 Phenolic, Nodular, Injection Molded PLENCO 04304 is a heat resistant, mineral filled phenolic molding compound offering improved mechanical strength properties along with excellent dimensional stability. UL recognized under component .. |
|||
Bulk Density | 0.670 g/cc | 0.0242 lb/in³ | Poured; ASTM D1895 |
Eastman Eastar A150 Copolyester, Film Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethan.. |
|||
Bulk Density | 0.670 g/cc | 0.0242 lb/in³ | |
DuPont™ Nomex® E56 Paper, 10 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Bulk Density | 0.670 g/cc | 0.0242 lb/in³ | |
DuPont™ Nomex® E56 Paper, 12 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Bulk Density | 0.670 g/cc | 0.0242 lb/in³ | |
DuPont™ Nomex® E56 Paper, 15 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Bulk Density | 0.670 g/cc | 0.0242 lb/in³ | |
DuPont™ Nomex® E56 Paper, 20 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Bulk Density | 0.670 g/cc | 0.0242 lb/in³ | ASTM D1895 |
ALM PA 605-A Filled Nylon 12 Prototyping Polymer 50% Aluminum filled nylon 12 that can produce accurate parts with excellent part strength and surface detail.Drop in replacement for other commercially available 50% aluminum filled materials with a.. |
|||
Bulk Density | 0.670 g/cc | 0.0242 lb/in³ | ISO 60 |
Vyncolit W5020 Glass Filled Novolac Phenolic Novolac resin based, glass fiber and glass bead reinforced. High dimensional stability and excellent chemical resistance at high temperatures in hydraulic brake fluids. Used in the ABS system.Inform.. |
|||
Bulk Density | 0.670 g/cc | 0.0242 lb/in³ | ASTM D1895 |
ALM PA-615-GS Filled Nylon 12 Prototyping Polymer 50% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.Drop-in replacement for other commercially .. |
|||
Bulk Density | 0.670 g/cc | 0.0242 lb/in³ | ASTM D1895 |
Plenco 7552 Phenolic, Nodular, Injection Molded PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re.. |