Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | Loose |
Nyco NYAD® M325 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | Loose |
Nyco NYAD® MD325 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | Loose |
Nyco NYGLOS® STPO Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | |
Nabaltec APYRAL® 16 Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | |
Nabaltec APYRAL® 4 Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | |
Nabaltec NABALOX® NO 135 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | |
Nabaltec APYRAL® 8 Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Bulk Density | <= 0.750 g/cc | <= 0.0271 lb/in³ | |
Magyar Aluminum ALOLT 710 Aluminum Hydroxide Viscosity Optimized Type |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | |
Solvay JAGUAR® EXCEL Surfactant Description: Clear grade with excellent wet combing and detangling benefits. Recommended for use in a broad range of conditioning shampoos.Chemical Name: Guar Gum DerivativeC.T.F.A./I.N.C.I. Name: G.. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | Powder Density; ASTM D1895 |
Sumitomo Bakelite North America E 3938A Hardware Grade Epoxy Fiberglass reinforced epoxy molding compound with excellent dimensional stability, good strength and excellent electrical insulation properties.Information provided by Vyncolit, a Sumitomo Bak Group.. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | Powder Density; ASTM D1895 |
Sumitomo Bakelite North America RX® 1-520/RX® 1310 Short-Glass Reinforced Diallyl Phthalate Short glass fiber reinforced, non-flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type SDG.Information provided by Vyncolit, a Sumitomo Bak Group.. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | ISO 60 |
Sumitomo Bakelite North America RX® 613 Fiberglass Reinforced Phenolic RX 613 is a fiberglass reinforced phenolic molding compound with good dimensional stability and good strength at elevated temperatures.Information provided by Sumitomo Bak North America, Inc. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | Powder; ASTM D1895 |
Sumitomo Bakelite North America FM 4005X4648 Fiberglass Reinforced Phenolic Novolac FM 4005X4648 a fiberglass reinforced phenolic novolac molding compound formulated to increase thermal conductivity and electrical conductance. This material also exhibits low post mold shrinkage.In.. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | |
Solvay RHODOPOL® 23 Surfactant Description: Rhodopol® 23 is Standard grade Xanthan Gum. It exhibits high pseudoplastic behavior and rapid hydration rate. This grade is registered on the FALCON list of approved substances.Ident.. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | ASTM D1895 |
Plenco 6401 Phenolic, Briquette, Transfer Molded PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | Tap |
TIMCAL TIMREX® M100 mesh FR Natural Flake Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | Powder Density; ISO 60 |
Vyncolit 2940 W Novolac Phenolic Mineral and glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. USES: Multi-V pulleys and solenoid covers.Information provided by Vyncolit, a Sumitomo Bak .. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | Powder Density; ISO 60 |
Vyncolit X620/1 Novolac Phenolic Glass fiber and graphite filled phenolic molding compound with excellent friction properties.USES: Low friction bearings, video recorder and compact disc parts. Not suitable for applications requir.. |
|||
Bulk Density | 0.750 - 0.850 g/cc | 0.0271 - 0.0307 lb/in³ | Powder Density; ISO 60 |
Vyncolit 2920 W Novolac Phenolic Mineral and organic filled molding compound with good dimensional stability and heat resistance.USES: Carburettor and intake manifold thermal insulator.Information provided by Vyncolit, a Sumitomo B.. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | ISO 60 |
Vyncolit BXE650 Inorganic Filled Phenolic Molding Compound Novolac resin based, inorganic filled. Excellent isotropic properties and superior dimensional stability. High mechanical properties even at elevated temperaturesInformation provided by Sumitomo Bak.. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | |
DuPont™ Nomex® N196 Paper, 2 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |
|||
Bulk Density | >= 0.750 g/cc | >= 0.0271 lb/in³ | |
Chosun Refractories A-7 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | Internal |
Eurostar Starpylen HU 70E4 ECR Starpylen HU 70E4 ECR is a Renewable Calcium Carbonate (oyster shell) Masterbatch in a PP carrier. Engineered to reduce carbon footprint in mineral filled compound.Information provided by Eurostar. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | |
Daikin NEOFLON ACX-31 PFA Coating Powder, White NEOFLON PFA coating powder is designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 30-80 micron thickness.Processing Methods: Electrostati.. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | |
Daikin NEOFLON ACX-34 PFA Coating Powder, White NEOFLON PFA coating powder is designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 30-80 micron thickness.Processing Methods: Electrostati.. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | |
Daikin NEOFLON NC-1830 FEP Coating Powder, Gray NEOFLON FEP coating powders are designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 0.5-5 mm thickness.Processing Methods: Roto lining.In.. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | |
Asahi Glass Fluon® G307 PTFE Granular Powder Fluon®PTFE granular powders (molding powders) are used for the production of sheets, rods, billets and other general moldings.Information provided by Asahi Glass Company, Inc. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | ASTM D1895 |
ALM PA-616-GS Filled Nylon 12 Prototyping Polymer 50% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.The PA 616-GS can be processed on any laser.. |
|||
Bulk Density | 0.750 g/cc | 0.0271 lb/in³ | Powder; ASTM D1895 |
Sumitomo Bakelite North America FM 4005X4649 Fiberglass Reinforced Phenolic Novolac FM 4005X4649 a fiberglass reinforced two-step phenolic molding compound formulated to increase thermal conductivity, to provide static dissipation and good wear resistance to abrasive media.Informat.. |