Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.818 g/cc | 0.0296 lb/in³ | Poured; ASTM D1895 |
Eastman Vitiva PC715 PET
(discontinued **) Vitiva PET PC715 is an exceptionally clear PET polyester that contains a UV light protection package chemically bound to the backbone of the polymer. This non-extractable UV inhibitor absorbs damagi.. |
|||
Bulk Density | 0.820 g/cc | 0.0296 lb/in³ | ASTM D1895 |
Eastman GP800 PET
(discontinued **) Voridian PET GP800 is a general purpose polymer that is available in the European, Middle East and Africa region. This product is developed for optimal production of PET bottles, containers, and fil.. |
|||
Bulk Density | 0.820 g/cc | 0.0296 lb/in³ | ASTM D4894 |
3M Dyneon™ TR 1105 PTFE
(discontinued **) Ideal for thin wall ram extrusion productsReduces cold flow and melt viscosityLower permeabilityLower porosityWeldableExcellent product smoothnessIncreased machine outputInformation provided by Dyne.. |
|||
Bulk Density | 0.820 g/cc | 0.0296 lb/in³ | ISO 60 |
FKuR Kunststoff Bio-Flex® A 4100 CL Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Bulk Density | 0.820 - 0.900 g/cc | 0.0296 - 0.0325 lb/in³ | |
SK Chemicals SKYPET® BB7755 Specially Formulated PET Resin Description: SKYPET-BB7755 is a specially formulated PET resin for PET bottles especially for hot-fill application. SKYPET-BB7755 provides excellent processability in injection molding and blow mol.. |
|||
Bulk Density | 0.820 - 0.900 g/cc | 0.0296 - 0.0325 lb/in³ | |
SK Chemicals SKYPET® BL8050 Specially Formulated PET Copolymer Resin SKYPET-BL8050 is a specially formulated PET copolymer resin for PET bottles and extruded sheet. SKYPET-BL8050 provides excellent processability in injection molding and blow molding processes, offe.. |
|||
Bulk Density | 0.820 - 0.900 g/cc | 0.0296 - 0.0325 lb/in³ | |
SK Chemicals SKYPET® BR8040 Low Content CHDM Modified Copolyester Resin Description: SKYPET-BR8040 is a low content CHDM modified copolyester resin for large sized-mineral water bottles and extruded sheet. SKYPET-BR8040 has sufficiently low crystallization rate for lar.. |
|||
Bulk Density | 0.820 - 0.900 g/cc | 0.0296 - 0.0325 lb/in³ | |
SK Chemicals SKYPET® XT8050 Specially Formulated PET Copolymer Resin Description: SKYPET-XT8050 is a fast reheat grade of SKYPET, specially formulated for high productivity in the blowing process. SKYPET-XT8050 provides excellent processability in injection molding .. |
|||
Bulk Density | 0.820 - 0.900 g/cc | 0.0296 - 0.0325 lb/in³ | |
SK Chemicals SKYPET® BB8055 Specially Formulated PET Resin Description: SKYPET-BB8055 is a specially formulated PET resin for PET bottles especially for hot-fill application. SKYPET-BB8055 provides excellent processability in injection molding and blow mol.. |
|||
Bulk Density | 0.820 - 0.900 g/cc | 0.0296 - 0.0325 lb/in³ | |
SK Chemicals SKYPET® BL8450 Specially Formulated PET Copolymer Resin Description: SKYPET-BL8450 is a specially formulated PET copolymer resin for PET bottles and extruded sheet. SKYPET-BL8450 provides excellent processability in injection molding and blow molding pr.. |
|||
Bulk Density | 0.820 g/cc | 0.0296 lb/in³ | ASTM D1895 |
Plenco 1501 Polyester, Pellet, Injection Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Bulk Density | 0.820 g/cc | 0.0296 lb/in³ | Tap |
TIMCAL TIMREX® 50X80 mesh Natural Flake Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Bulk Density | 0.820 g/cc | 0.0296 lb/in³ | |
DuPont™ Nomex® N196 Paper, 10 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |
|||
Bulk Density | 0.820 g/cc | 0.0296 lb/in³ | |
DuPont™ Nomex® N196 Paper, 7 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |
|||
Bulk Density | 0.820 g/cc | 0.0296 lb/in³ | |
Asahi Glass Fluon® G340 PTFE Granular Powder Fluon®PTFE granular powders (molding powders) are used for the production of sheets, rods, billets and other general moldings.Information provided by Asahi Glass Company, Inc. |