Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.900 - 1.10 g/cc | 0.0325 - 0.0397 lb/in³ | |
Magyar Aluminum ALO-B15 Alumina Calcined Alumina; Minimum 5% alpha-Al2O3. |
|||
Bulk Density | <= 0.900 g/cc | <= 0.0325 lb/in³ | |
Magyar Aluminum ALOLT 730 Aluminum Hydroxide Viscosity Optimized Type |
|||
Bulk Density | 0.900 - 1.10 g/cc | 0.0325 - 0.0397 lb/in³ | |
Magyar Aluminum ALO-P90 Alumina Alumina for Polishing |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ISO 60 |
Lanxess Pocan® DP 7102 000000 PBT, 32% Mineral PBT, 32% mineral, injection molding, LDSInformation provided by LANXESS. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ISO 60 |
Lanxess Pocan® DP 7318 000000 PBT, 17% Pigment PBT, 17% white pigments, injection molding, improved light reflection, low tendency to warpInformation provided by LANXESS. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ISO 60 |
Lanxess Pocan® T 7141 000000 PET + PBT, 40% Glass Fiber/Mineral PET + PBT, 40% glass fibers/mineral, injection molding, improved flowability, high thermal dimensional stabilityInformation provided by LANXESS. |
|||
Bulk Density | 0.900 - 1.20 g/cc | 0.0325 - 0.0434 lb/in³ | |
Solvay Chemicals Oxyper® S131 Sodium Percarbonate Oxyper® S131 is a stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in bleach additive products and environmental applications; it may be suitabl.. |
|||
Bulk Density | 0.900 - 1.20 g/cc | 0.0325 - 0.0434 lb/in³ | |
Solvay Chemicals Oxyper® S142 Sodium Percarbonate Oxyper® S142 is a stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in formulated bleach additive products, detergent powders and tablets, automa.. |
|||
Bulk Density | 0.900 - 1.20 g/cc | 0.0325 - 0.0434 lb/in³ | |
Solvay Chemicals Oxyper® SHC Sodium Percarbonate Oxyper® SHC is a high coated, stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in bleach additive products, detergent powders and tablets, autom.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | |
Sharadaa Ceramics 26 Insulation Bricks-ASTM Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | |
Sharadaa Ceramics HFI Insulation Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFINSUL 8S Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America Epiall® 1904B-1 Short Glass Fiber Reinforced Epoxy Epiall 1904B-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided .. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | Powder; ISO 60 |
Sumitomo Bakelite North America RX® 660 Fiberglass Reinforced Phenolic Novolac RX 660 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type MFH.Information supplied by Sumitom.. |
|||
Bulk Density | <= 0.900 g/cc | <= 0.0325 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFINSUL ZAP-015 Insulating Castables Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America Epiall® 1908B-1 Short Glass Fiber Reinforced Epoxy Epiall 1908B-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided .. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America SI 9550 Silicone Compound SI 9550 is a short fiberglass reinforced silicone molding compound, which offers moderate strength properties, and dimensional stability and excellent long-term thermal stability at elevated tempera.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1895 |
Plenco 05118-T5 Phenolic, Granular, Compression Molded PLENCO 05118-T5 is a mineral and graphite filled novolac phenolic molding compound with PTFE, formulated for bearing seals. 05118 provides for a low coefficient of friction, good wear resistance, ve.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | |
A. Schulman POLYBATCH™ White B8750A Concentrate Based In HDPE DescriptionPOLYBATCH® B8750A is a specialty white masterbatch based in HDPE. This product has been designed to achieve optimum dispersion and excellent letdown mixing in blow molding applications... |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | Tap |
TIMCAL TIMREX® FC250-1500 Coke TIMREX Petroleum Coke is calcined at appropriate temperature with low ash and sulfur (sulphur) content, well defined texture and consistent particle size distribution.Advantages and applications: S.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | Size D (tapped) |
Vesta Ceramics SicoMill® Grade 2 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | |
A. Schulman POLYBATCH™ White B8750A Concentrate Based In HDPE DescriptionPOLYBATCH® B8750A is a specialty white masterbatch based in HDPE. This product has been designed to achieve optimum dispersion and excellent letdown mixing in blow molding applications... |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | |
A. Schulman POLYBATCH™ White B8750A Concentrate Based In HDPE DescriptionPOLYBATCH® B8750A is a specialty white masterbatch based in HDPE. This product has been designed to achieve optimum dispersion and excellent letdown mixing in blow molding applications... |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D894 |
Daikin POLYFLON M-139 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding and automatic compression molding.Features: Excellent fluidity. Apparent density is large and ideal for automated compression molding proces.. |
|||
Bulk Density | >= 0.900 g/cc | >= 0.0325 lb/in³ | |
Chosun Refractories B-6 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | |
BASF Sicotan® Brown K 2711 Color Additive Chemical Structure: Mn/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: B.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America Epiall® 1914A Short Glass Fiber Reinforced Epoxy Epiall 1914A is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided by.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America Epiall® 1961B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy Epiall 1961B-1 is a short glass fiber and mineral filled epoxy molding compound with excellent dimensional stability, good strength properties, and good electrical insulation properties.Information .. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | Powder Density; ASTM D1895 |
Sumitomo Bakelite North America SI 9002J-1 Silicone Compound SI 9002J-1 is a short fiberglass reinforced silicone molding compound, which offers moderate strength properties, and dimensional stability and excellent long-term thermal stability at elevated temp.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | |
A. Schulman POLYBATCH™ White B8750A Concentrate Based In HDPE DescriptionPOLYBATCH® B8750A is a specialty white masterbatch based in HDPE. This product has been designed to achieve optimum dispersion and excellent letdown mixing in blow molding applications... |