Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Bulk Density = 0.190 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.190 g/cc
0.00686 lb/in³
ASTM D1895
Kraton® G1640 E (SEBS) Linear Triblock Copolymer
Description: Kraton G1640 E is a clear linear triblock copolymer based on styrene and ethylene/butylene (S-E/B-S) with bound styrene of 32.9% mass. It is supplied from Europe as identified in the gr..
Bulk Density 0.190 g/cc
0.00686 lb/in³
EN ISO 60
Gwent Electronic Materials P2121112P11 Oxygen Plasma Modified Multiwalled Carbon Nanotubes
Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Bulk Density 0.190 g/cc
0.00686 lb/in³
EN ISO 60
Gwent Electronic Materials P2121112P12 Acid Vapor Plasma Modified Single and Double Walled Carbon Nanotubes
Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Bulk Density 0.190 g/cc
0.00686 lb/in³
EN ISO 60
Gwent Electronic Materials P2121112P13 Argon Plasma Modified Single and Double Walled Carbon Nanotubes
Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Bulk Density 0.190 g/cc
0.00686 lb/in³
EN ISO 60
Gwent Electronic Materials P2121112P14 Nitrogen Plasma Modified Single and Double Walled Carbon Nanotubes
Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Bulk Density 0.190 g/cc
0.00686 lb/in³
EN ISO 60
Gwent Electronic Materials P2121112P15 Ammonia Plasma Modified Single and Double Walled Carbon Nanotubes
Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Bulk Density 0.190 g/cc
0.00686 lb/in³
EN ISO 60
Gwent Electronic Materials P2121112P16 Oxygen Plasma Modified Single and Double Walled Carbon Nanotubes
Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Bulk Density 0.190 g/cc
0.00686 lb/in³
EN ISO 60
Gwent Electronic Materials P2121112P18 Nitrogen Plasma Modified Multiwalled Carbon Nanotubes
Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Bulk Density 0.190 g/cc
0.00686 lb/in³
EN ISO 60
Gwent Electronic Materials P2121112P19 Tetrafluoromethane Plasma modified Single and Double Walled Carbon Nanotubes
Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Bulk Density 0.190 g/cc
0.00686 lb/in³
EN ISO 60
Gwent Electronic Materials P2121112P7 Acid Vapor Plasma Modified Multiwalled Carbon Nanotubes
Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Bulk Density 0.190 g/cc
0.00686 lb/in³
EN ISO 60
Gwent Electronic Materials P2121112P8 Argon Plasma Modified Multiwalled Carbon Nanotubes
Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Bulk Density 0.190 g/cc
0.00686 lb/in³
EN ISO 60
Gwent Electronic Materials P2121112P9 Tetrafluoromethane Plasma Modified Multiwalled Carbon Nanotubes
Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Bulk Density 0.190 g/cc
0.00686 lb/in³
EN ISO 60
Gwent Electronic Materials P2121112P10 Ammonia Plasma Modified Multiwalled Carbon Nanotubes
Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Bulk Density 0.190 g/cc
0.00686 lb/in³
Scott
TIMCAL TIMREX® KC44 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Bulk Density 0.190 g/cc
0.00686 lb/in³
Scott, Typical
TIMCAL TIMREX® KS44 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Bulk Density 0.190 g/cc
0.00686 lb/in³
Scott
TIMCAL TIMREX® SFG44 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Bulk Density 0.190 g/cc
0.00686 lb/in³
Scott, Typical
TIMCAL TIMREX® C-LUB 310 Primary Synthetic Graphite
Information provided by TIMCAL
Bulk Density 0.190 - 0.260 g/cc
0.00686 - 0.00939 lb/in³
Zircar Ceramics ASQ Castertip
14 pcf density refractory ceramic fiber "soft tip". Alumina bonding of shot free fiber results in extreme performance in manufacture of the finest grades of medical, food and packaging foils. Inform..
Copyright © lookpolymers.com All Rights Reserved