Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.270 g/cc | 0.00975 lb/in³ | |
Potters Industries Q-Cel® 6048 Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat.. |
|||
Bulk Density | 0.270 g/cc | 0.00975 lb/in³ | |
Zircar Zirconia CeF-100 Ceria Felt Insulation Ceria (cerium dioxide), CeO2, has a very high surface area and is ideal as a catalyst support. Our ceria fibers and textiles are made by the same unique Zircar process used for manufacturing yttria-.. |
|||
Bulk Density | 0.270 g/cc | 0.00975 lb/in³ | Tap Density |
Momentive Performance Materials PolarTherm® PT100 Boron Nitride (BN) Powder Single crystal platelet BN Powder. High aspect ratio platelets may improve thermal conductivity when used as a filler in polymers or lubricants. Features of BN include thermal conductor, electrica.. |
|||
Bulk Density | 0.270 g/cc | 0.00975 lb/in³ | |
Zircar Zirconia CeF-100 Ceria Felt Insulation Ceria (cerium dioxide), CeO2, has a very high surface area and is ideal as a catalyst support. Our ceria fibers and textiles are made by the same unique Zircar process used for manufacturing yttria-.. |
|||
Bulk Density | 0.270 g/cc | 0.00975 lb/in³ | |
Zircar Zirconia ZYBF-4 Zirconia Bulk Fiber Insulation Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed .. |
|||
Bulk Density | 0.270 g/cc | 0.00975 lb/in³ | |
Zircar Zirconia ZYBF-4 Zirconia Bulk Fiber Insulation Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed .. |