Polymer Property : Bulk Density = 0.670 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.670 g/cc
0.0242 lb/in³
Zircar Zirconia CeW-15 Ceria Woven Textile Insulation
Ceria (cerium dioxide), CeO2, has a very high surface area and is ideal as a catalyst support. Our ceria fibers and textiles are made by the same unique Zircar process used for manufacturing yttria-..
Bulk Density 0.670 g/cc
0.0242 lb/in³
Zircar Zirconia CeW-30 Ceria Woven Textile Insulation
Ceria (cerium dioxide), CeO2, has a very high surface area and is ideal as a catalyst support. Our ceria fibers and textiles are made by the same unique Zircar process used for manufacturing yttria-..
Bulk Density 0.670 g/cc
0.0242 lb/in³
Struktol ZINC STEARATE CM
A clear melt zinc stearate, is manufactured from high quality stearic acid in a tightly controlled production operation that guarantees product uniformity.STRUKTOL® Zinc Stearate CM, a clear melt..
Bulk Density 0.670 g/cc
0.0242 lb/in³
ASTM D1895
Plenco 00732 Melamine-Phenolic, Granular, Compression Molded
PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 007..
Bulk Density 0.670 g/cc
0.0242 lb/in³
ASTM D1895
Plenco 00732 Melamine-Phenolic, Granular, Injection Molded
PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 007..
Bulk Density 0.670 g/cc
0.0242 lb/in³
ASTM D1895
Plenco 3509 Phenolic, Granular, Injection Molded
PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file..
Bulk Density 0.670 g/cc
0.0242 lb/in³
ASTM D1895
Plenco 6582 Phenolic, Briquette, Injection Molded
PLENCO 06582 is a rubber modified phenolic molding compound, offering excellent heat resistant properties, along with improved mechanical strength at elevated temperatures. UL recognized under compo..
Bulk Density 0.670 g/cc
0.0242 lb/in³
Scott
TIMCAL TIMREX® KS150-600SP Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Bulk Density 0.670 g/cc
0.0242 lb/in³
ISO 60
Vyncolit X7255 Glass Fiber Reinforced Novolac Phenolic
Novolac resin based, glass fiber and glass beads reinforced. Very easy to transform in complex shapes. Excellent mechanical and thermal properties. Higher isotropic properties and good dimensional s..
Bulk Density 0.670 g/cc
0.0242 lb/in³
Zircar Zirconia CeW-15 Ceria Woven Textile Insulation
Ceria (cerium dioxide), CeO2, has a very high surface area and is ideal as a catalyst support. Our ceria fibers and textiles are made by the same unique Zircar process used for manufacturing yttria-..
Bulk Density 0.670 g/cc
0.0242 lb/in³
Zircar Zirconia CeW-30 Ceria Woven Textile Insulation
Ceria (cerium dioxide), CeO2, has a very high surface area and is ideal as a catalyst support. Our ceria fibers and textiles are made by the same unique Zircar process used for manufacturing yttria-..
Bulk Density 0.670 g/cc
0.0242 lb/in³
ASTM D1895
Plenco 4304 Phenolic, Nodular, Injection Molded
PLENCO 04304 is a heat resistant, mineral filled phenolic molding compound offering improved mechanical strength properties along with excellent dimensional stability. UL recognized under component ..
Bulk Density 0.670 g/cc
0.0242 lb/in³
Poured; ASTM D1895
Eastman Eastar A150 Copolyester, Film
Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethan..
Bulk Density 0.670 g/cc
0.0242 lb/in³
DuPont™ Nomex® E56 Paper, 10 mil Nominal Thickness
Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as..
Bulk Density 0.670 g/cc
0.0242 lb/in³
DuPont™ Nomex® E56 Paper, 12 mil Nominal Thickness
Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as..
Bulk Density 0.670 g/cc
0.0242 lb/in³
DuPont™ Nomex® E56 Paper, 15 mil Nominal Thickness
Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as..
Bulk Density 0.670 g/cc
0.0242 lb/in³
DuPont™ Nomex® E56 Paper, 20 mil Nominal Thickness
Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as..
Bulk Density 0.670 g/cc
0.0242 lb/in³
ASTM D1895
ALM PA 605-A Filled Nylon 12 Prototyping Polymer
50% Aluminum filled nylon 12 that can produce accurate parts with excellent part strength and surface detail.Drop in replacement for other commercially available 50% aluminum filled materials with a..
Bulk Density 0.670 g/cc
0.0242 lb/in³
ISO 60
Vyncolit W5020 Glass Filled Novolac Phenolic
Novolac resin based, glass fiber and glass bead reinforced. High dimensional stability and excellent chemical resistance at high temperatures in hydraulic brake fluids. Used in the ABS system.Inform..
Bulk Density 0.670 g/cc
0.0242 lb/in³
ASTM D1895
ALM PA-615-GS Filled Nylon 12 Prototyping Polymer
50% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.Drop-in replacement for other commercially ..
Bulk Density 0.670 g/cc
0.0242 lb/in³
ASTM D1895
Plenco 7552 Phenolic, Nodular, Injection Molded
PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re..