Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | Tapped |
Nyco M3 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | |
Nabaltec NABALOX® NO 325 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | PEPL-10-W-67 |
Pearl Engineering PEPLPET F097H Film Grade Resin Used mainly as PET films/ sheets, known as Superbright |
|||
Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | PEPL-10-W-67 |
Pearl Engineering PEPLPET F097HA Film Grade Resin Used mainly as PET films/ sheets, known as bright with anti-blocking agent. |
|||
Bulk Density | 0.700 - 1.00 g/cc | 0.0253 - 0.0361 lb/in³ | |
Magyar Aluminum ALO-DFM Alumina Alumina for Polishing |
|||
Bulk Density | 0.700 - 0.950 g/cc | 0.0253 - 0.0343 lb/in³ | |
Magyar Aluminum ALO-P54 Alumina Alumina for Polishing |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers PA 66, 15% glass fibers, injection molding, heat-ageing stabilized |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Durethan® AKV 30 000000 Nylon 66, Glass Fiber Reinforced PA 66, 30% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Durethan® BG 30 X H3.0 000000 Nylon 6, 30% Glass Fibers/Glass Spheres PA 6, 30% glass fibers/glass spheres, injection molding, heat-ageing stabilized, low tendency to warp |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Durethan® BKV 230 H3.0 000000 Nylon 6-Copolymer, 30% Glass Fibers PA 6-Copolymer, 30% glass fibers, injection molding, impact modified, heat-ageing stabilized |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, halogen free flame retardant.Information provided by LANXESS. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | |
Lucite International Colacryl ® CRG107 Specialty Acrylic Resin Colacryl® CRG107 is a hard, methyl methacrylate based, acrylic resin with exceptional pigment wetting properties. It is soluble in chlorinated hydrocarbons, ketones and lower esters and compatibl.. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | Apparent Density |
Indium Corp. Ga2O3 Gallium Sesquioxide Synonyms: Gallium Oxide, Gallium (III) OxideCAS Number: 12024-21-4EC Number: 234-691-7RTECS: LW9650000Purity: 99.99 to 99.999% Gallium SesquioxideAppearance/Form: White powderCrystal structure.. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Durethan® ECO BV 30 H2 900500 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, heat-ageing stabilized, contains 30% pre-consumer recycled materialInformation provided by LANXESS. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | |
Solvay JAGUAR® C 14 S Surfactant Description: Substantive to hair and skin. Provides excellent wet combing and soft non-tacky feel to hair.Chemical Name: Guar Gum DerivativeC.T.F.A./I.N.C.I. Name : GUAR HYDROXYPROPYLTRIMONIUM CHLOR.. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | |
Solvay JAGUAR® HP 8 COS Surfactant Description: Hydroxypropyl Guar for thickening, which provides a fluid and smooth wet feel to formulationsChemical Name: Guar Gum DerivativeC.T.F.A./I.N.C.I. Name: Hydroxypropyl GuarCAS: 39421-75-5S.. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Sumikon® PM-6430 Glass-Filled Phenolic, Injection Grade Sumikon PM-6430 black Phenolic is a two stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s.. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | Powder Density; ISO 60 |
Vyncolit 4523 XB Novolac Phenolic Organic and inorganic filled phenolic molding compound with good mechanical and thermal properties. Improved heat resistance compared to organic filled compounds.USES: Fuse holders, brush holders, .. |
|||
Bulk Density | 0.700 - 0.850 g/cc | 0.0253 - 0.0307 lb/in³ | Powder Density; ISO 60 |
Vyncolit G885 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | Powder Density; ISO 60 |
Vyncolit G865 Novolac Phenolic Glass fiber filled phenolic molding compound with high mechanical, good thermal and electrical properties. USES: Asbestos-free replacement for die-cast automotive metal parts, e.g. reactors for aut.. |
|||
Bulk Density | >= 0.700 g/cc | >= 0.0253 lb/in³ | |
Chosun Refractories B-1 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | >= 0.700 g/cc | >= 0.0253 lb/in³ | |
Chosun Refractories B-2 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU Information provided by BASF |
|||
Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
BASF Ultrason® E 3010 MR UN PESU Description: Unreinforced, higher viscosity injection molding and extrusion grade with improved toughness and chemical resistance (stress crack resistance); demolding optimized. Abbreviated designat.. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | |
3M Dyneon™ Dynamar™ FX 9614 Polymer Processing Additive Dynamar polymer processing additive FX 9614 is a free flowing granular concentrate form of a fluoropolymer designed for use at very low levels to improve the processing of thermoplastics. At the ver.. |
|||
Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
BASF Ultrason® S 3010 MR UN PSU Description: Unreinforced, higher viscosity injection molding and extrusion grade, tougher, with improved chemical resistance and demolding optimized. Abbreviated designation according to ISO 1043-1.. |
|||
Bulk Density | 0.700 - 0.850 g/cc | 0.0253 - 0.0307 lb/in³ | Powder Density; ISO 60 |
Vyncolit X682 Novolac Phenolic Glass fiber, glass bead and graphite filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction.USES: Water pump seals and self-lubricating bearings.Info.. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ASTM D1895 |
Plenco 00714 Melamine-Phenolic, Granular, Transfer Molded PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4.. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Sumikon® PM-6430 Glass-Filled Phenolic, Compression Grade Sumikon PM-6430 black Phenolic is a two stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional sta.. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | Powder Density; ISO 60 |
Sumitomo Bakelite North America RX® 852 Novolac Phenolic Fiberglass reinforced phenolic novolac compound with good dimensional stability and good strength at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group |