Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.910 g/cc | 0.0329 lb/in³ | Tapped |
Nyco M1250 AS WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Bulk Density | 0.910 g/cc | 0.0329 lb/in³ | Tapped |
Nyco M1250 ES WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.910 g/cc | 0.0329 lb/in³ | Tapped |
Nyco M1250 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Bulk Density | 0.910 g/cc | 0.0329 lb/in³ | Tapped |
Nyco MD1250 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.910 g/cc | 0.0329 lb/in³ | ASTM D1895 |
Plenco 05118-T5 Phenolic, Granular, Injection Molded PLENCO 05118-T5 is a mineral and graphite filled novolac phenolic molding compound with PTFE, formulated for bearing seals. 05118 provides for a low coefficient of friction, good wear resistance, ve.. |
|||
Bulk Density | 0.910 g/cc | 0.0329 lb/in³ | Tap |
TIMCAL TIMREX® FC250 Coke TIMREX Petroleum Coke is calcined at appropriate temperature with low ash and sulfur (sulphur) content, well defined texture and consistent particle size distribution.Advantages and applications: S.. |