Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.060 - 0.10 µm | 0.060 - 0.10 µm | outside diameter |
NanoAmor 95%, OD/ID: 60-100/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.070 - 0.10 µm | 0.070 - 0.10 µm | |
American Elements Aluminum Nanoparticles General DescriptionAluminum (Al) Nanoparticles, nanodots or Nanopowder are black spherical high surface area metal particles. Nanoscale Aluminum Particles are typically 10-30 nanometers (nm) with sp.. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Aluminum Nitride Nanoparticles General DescriptionAluminum Nitride (AlN) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Aluminum Nitride Particles are typically 10 - 100 nanometers (nm).. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Boron Carbide Nanoparticles General DescriptionBoron Carbide (BC) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Boron Carbide Particles are typically 10 - 100 nanometers (nm) with s.. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Boron Nitride Nanoparticles General DescriptionBoron Nitride (BN) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Boron Nitride Particles are typically 10 - 100 nanometers (nm) with s.. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Calcium Chloride Nanoparticles General DescriptionCalcium Chloride (CaCl) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Calcium Chloride Particles are typically 10 - 100 nanometers (nm.. |
|||
Particle Size | 0.020 - 0.10 µm | 0.020 - 0.10 µm | |
American Elements Gold Nanoparticles General DescriptionGold (Au) Nanoparticles, nanodots or nanopowder are brown spherical high surface area metal particles. Nanoscale Gold Particles are typically 20 - 100 nanometers (nm) with specifi.. |
|||
Particle Size | 0.020 - 0.10 µm | 0.020 - 0.10 µm | |
American Elements Iridium Nanoparticles General DescriptionIridium (Ir) Nanoparticles, nanodots or nanopowder are black spherical high surface area metal particles. Nanoscale Iridium Particles are typically 20 - 100 nanometers (nm) with s.. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Lithium Vanadate Nanoparticles General DescriptionLithium Vanadate or Lithium Vanadium Oxide (LiVO) Nanoparticles, nanodots or nanopowder are spinel, high surface area particles. Nanoscale Lithium Vanadate or Lithium Vanadium Oxi.. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Lutetium Nanoparticles General DescriptionLutetium (Lu) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Lutetium Particles are typically 10 - 100 nanometers (nm) with speci.. |
|||
Particle Size | 0.0050 - 0.10 µm | 0.0050 - 0.10 µm | |
American Elements Magnesium Oxide Nanopowder General DescriptionMagnesium Oxide Nanoparticles or Magnesia Nanoparticles (MgO) Nanoparticles, nanodots or nanopowder are spinel, high surface area particles. Nanoscale Magnesium Oxide Nanoparticle.. |
|||
Particle Size | 0.0050 - 0.10 µm | 0.0050 - 0.10 µm | |
American Elements Manganese Oxide Nanopowder General DescriptionManganese Oxide Nanopowder (MnO), nanodots or nanoparticles are high surface area particles. Nanoscale Manganese Oxide Nanoparticles are typically 5 - 100 nanometers (nm) with spe.. |
|||
Particle Size | 0.050 - 0.10 µm | 0.050 - 0.10 µm | |
American Elements Molybdenum Nanoparticles General DescriptionMolybdenum (Mo) Nanoparticles, nanodots or nanopowder are black high surface area particles. Nanoscale Molybdenum Particles are typically 50 - 100 nanometers (nm) with specific su.. |
|||
Particle Size | 0.050 - 0.10 µm | 0.050 - 0.10 µm | |
American Elements Nickel Nanoparticles General DescriptionNickel (Ni) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Nickel Particles are typically 10 - 40 nanometers (nm) with specific s.. |
|||
Particle Size | 0.050 - 0.10 µm | 0.050 - 0.10 µm | |
American Elements Nickel Titanium Nanoparticles General DescriptionNickel Titanium (NiTi) Nanoparticles, nanodots or nanopowder are black spherical high surface area alloy particles. Nanoscale Nickel Titanium Particles are typically 10 - 40 nanom.. |
|||
Particle Size | 0.020 - 0.10 µm | 0.020 - 0.10 µm | |
American Elements Niobium Oxide Nanoparticles General DescriptionNiobium Oxide ( MoO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Na.. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Palladium Nanoparticles General DescriptionPalladium (Pd) Nanoparticles, nanodots or nanopowder are black spherical high surface area metal particles. Nanoscale Palladium Particles are typically 20 - 100 nanometers (nm) wi.. |
|||
Particle Size | 0.020 - 0.10 µm | 0.020 - 0.10 µm | |
American Elements Platinum Nanoparticles General DescriptionPlatinum (Pt) Nanoparticles, nanodots or nanopowder are brown spherical high surface area metal particles. Nanoscale Platinum Particles are typically 20 - 100 nanometers (nm) with.. |
|||
Particle Size | 0.020 - 0.10 µm | 0.020 - 0.10 µm | |
American Elements Rhenium Nanoparticles General DescriptionRhenium (Re) Nanoparticles, nanodots or nanopowder are brown spherical high surface area metal particles. Nanoscale Rhenium Particles are typically 20 - 100 nanometers (nm) with s.. |
|||
Particle Size | 0.020 - 0.10 µm | 0.020 - 0.10 µm | |
American Elements Ruthenium Nanoparticles General DescriptionRuthenium (Ru) Nanoparticles, nanodots or nanopowder are brown spherical high surface area metal particles. Nanoscale Ruthenium Particles are typically 20 - 100 nanometers (nm) wi.. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Silicon Nanotubes General DescriptionSilicon (Si) Nanotubes, Single-Walled, Double Walled and Multi-Walled are tubular ultra high surface area nanotubes. Nanoscale Silicon Nanotubes are typically 10 - 100 nanometers .. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Silicon Nitride Nanoparticles General DescriptionSilicon Nitride (SiN) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Silicon Nitride Particles are typically 10 - 100 nanometers (nm) w.. |
|||
Particle Size | 0.060 - 0.10 µm | 0.060 - 0.10 µm | |
American Elements Strontium Carbonate Nanoparticles General DescriptionStrontium Carbonate (SrCO3) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Strontium Carbonate Particles are typically 5 - 40 nan.. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Titanium Carbide Nanoparticles General DescriptionTitanium Carbide (TiC) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Titanium Carbide Particles are typically 10 - 100 nanometer.. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Tungsten Carbide Nanoparticles General DescriptionTungsten Carbide (TiC) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Tungsten Carbide Particles are typically 10 - 100 nanometer.. |
|||
Particle Size | 0.0050 - 0.10 µm | 0.0050 - 0.10 µm | |
American Elements Yttria stabilized Zirconia General DescriptionYttria stabilized Zirconia or Zirconium Oxide Nanopowder or Nanoparticles (YSZ), nanodots or nanocrystals are white high surface area particles available fully stabilized (8 mol%).. |
|||
Particle Size | 0.075 - 0.10 µm | 0.075 - 0.10 µm | |
American Elements Yttrium Nanoparticles General DescriptionYttrium (Y) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Yttrium Particles are typically 5 - 45 nanometers (nm) with specific s.. |
|||
Particle Size | 0.050 - 0.10 µm | 0.050 - 0.10 µm | |
American Elements Zirconium Nanoparticles General DescriptionZirconium (Zr) Nanoparticles, nanodots or Nanopowder are black spherical high surface area metal particles. Nanoscale Zirconium Particles are typically 10-40 nanometers (nm) with .. |
|||
Particle Size | 0.0050 - 0.10 µm | 0.0050 - 0.10 µm | |
American Elements Zirconium Oxide Nanopowder General DescriptionZirconium Oxide or Zirconia Nanopowder or Nanoparticles (ZrO2), nanodots or nanocrystals are white high surface area particles available in monoclinic or as stabilized or doped wi.. |
|||
Particle Size | 0.060 - 0.10 µm | 0.060 - 0.10 µm | |
American Elements Cerium Nanoparticles General DescriptionCerium (Ce) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Cerium Particles are typically 5 - 40 nanometers (nm) with specific su.. |