Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.80 µm | 0.80 µm | Median Diameter |
Omya OMYAPAQUE® Calcium Carbonate An ultrafine ground calcium carbonate for paper and board filling. An opacifying product that is designed to reduce costs through the replacement of more expensive pigments.Information supplied by O.. |
|||
Particle Size | 0.80 - 1.5 µm | 0.80 - 1.5 µm | d50 |
Magyar Aluminum ALOLT 120F Aluminum Hydroxide Fine Precipitated Type |
|||
Particle Size | 0.80 µm | 0.80 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade HD 15 Boron Carbide, B4C Powder for sintering.Abrasive grit or powder (grinding, lapping, polishing)Wear resistant engineering components (e.g. sand-blasting and water jet nozzlesLight weight ceramic armorMetal infiltration.. |
|||
Particle Size | 0.80 µm | 0.80 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade HS Boron Carbide, B4C Powder for sintering.Abrasive grit or powder (grinding, lapping, polishing)Wear resistant engineering components (e.g. sand-blasting and water jet nozzlesLight weight ceramic armorMetal infiltration.. |
|||
Particle Size | 0.80 - 1.1 µm | 0.80 - 1.1 µm | d10 |
Indium Corp. In(OH)3 Fine Indium Hydroxide Indium Acetate is a white powder. Fine Powder Form: Primary particles range from 0.1 to 1.0 microns in size. they range in shape from spherical to elliptical to cylindrical. Agglomerates can be .. |
|||
Particle Size | 0.80 - 1.8 µm | 0.80 - 1.8 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade C Aluminum Nitride AIN High thermally conductive ceramicsComposite ceramicsSiAlONsHeat sinksElectrically insulating packages for electronicsCrucibles for metals and salt meltsThermally conductive filler for polymersCompon.. |
|||
Particle Size | 0.80 - 1.2 µm | 0.80 - 1.2 µm | Average |
H.C. Starck Grade C Titanium Nitride Additive for ceramic parts to increase electrical conductivityConstituent for cermets and black ceramicsRaw material for TiN sputter targets |
|||
Particle Size | 0.80 µm | 0.80 µm | |
Solvay Chemicals Blanc fixe brilliant Blanc Fixe Brilliant is the optimal extender for almost all applications in the production of paints and coatings and plastic.Information provided by Solvay |
|||
Particle Size | 0.80 µm | 0.80 µm | |
Shin-Etsu Silicones X-52-854 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Particle Size | 0.80 µm | 0.80 µm | Rubber Particle Size |
UBE B (Low-Cis) HIPS (n-DM = 0.03 wt % and PH-3H = 0.03 wt %) Description: UBE high impact polystyrene (HIPS).Information provided by UBE. |
|||
Particle Size | 0.80 µm | 0.80 µm | d10 |
TIMCAL TIMREX® HSAG400 Primary Synthetic High Surface Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 0.80 µm | 0.80 µm | d10 |
TIMCAL TIMREX® HSAG500 Primary Synthetic High Surface Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 0.80 µm | 0.80 µm | Rubber Particle Size |
UBE UBEPOL BR13HB HIPS (n-DM = 0.03 wt % and PH-3H = 0.03 wt %) Description: UBEPOL-BR13HB is characterized by its low solution viscosity compared with conventional grades and short dissolution time in styrene monomer. Its main merits are as follows:Short dissol.. |
|||
Particle Size | 0.80 µm | 0.80 µm | |
China Tungsten YG11X Tungsten Carbide Powder Information provided by China Tungsten |
|||
Particle Size | 0.80 µm | 0.80 µm | |
China Tungsten YG13X Tungsten Carbide Powder Information provided by China Tungsten |
|||
Particle Size | 0.80 µm | 0.80 µm | |
China Tungsten YG9X Tungsten Carbide Powder Information provided by China Tungsten |
|||
Particle Size | 0.80 µm | 0.80 µm | |
China Tungsten YG15X Tungsten Carbide Powder Information provided by China Tungsten |
|||
Particle Size | 0.80 µm | 0.80 µm | |
China Tungsten YG6X Tungsten Carbide Powder Information provided by China Tungsten |