Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | >= 1.5 µm | >= 1.5 µm | Primary Crystal Size |
Nabaltec NABALOX® NO 615-30 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | 1.5 - 2.5 µm | 1.5 - 2.5 µm | |
Nabaltec NABALOX® NO 625-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | >= 1.5 µm | >= 1.5 µm | Primary Crystal Size |
Nabaltec NABALOX® NO 625-30 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | >= 1.5 µm | >= 1.5 µm | Primary Crystal Size |
Nabaltec NABALOX® NO 625-31 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | 1.5 µm | 1.5 µm | |
Polyplastic Armoflen® PO MF 65-1 Linear Low Density Polyethylene, 65% Calcium Carbonate Information provided by PolyPlastic Group. |
|||
Particle Size | 1.5 µm | 1.5 µm | |
Polyplastic Armoflen® PO MF 65-2 Linear Low Density Polyethylene, 65% Calcium Carbonate Information provided by PolyPlastic Group. |
|||
Particle Size | 1.5 µm | 1.5 µm | mean aggregate size |
NanoScale NanoActive® Aluminum Oxide NanoActive Al2O3 is produced using proprietary processes to obtain high specific surface area, low density, amorphous material with high adsorption capacity and chemical reactivity. NanoActive Al2O3.. |
|||
Particle Size | 1.5 µm | 1.5 µm | Median Grain Diameter |
Nabaltec APYRAL® 40 VS1 Al(OH)3 The high quality and performance of our surface treated APYRAL® 40VS1 and APYRAL® 60VS1 powders complete the APRYAL® product range for highly specialized applications. Examples include, excellent.. |
|||
Particle Size | 1.5 µm | 1.5 µm | 50% of particles, (SRRG Powder) |
Ferro EG 0221 Specialty Glass Glass Type: MG-Al-Si (devitrified) Typical Powder Form: MVG, SRRG Typical Application: Sintering Aid / Ceramic Ferro offers a wide range of compositions for specialty applications including sinteri.. |
|||
Particle Size | 1.5 µm | 1.5 µm | 50% of particles, (SRRG Powder) |
Ferro EG 0225 Specialty Glass Glass Type: MG-Al-Si (devitrified) Typical Powder Form: MVG, SRRG Typical Application: Sintering Aid / Ceramic Ferro offers a wide range of compositions for specialty applications including sinteri.. |
|||
Particle Size | 1.5 µm | 1.5 µm | 50% of particles, (SRRG Powder) |
Ferro IP 750 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 1.5 µm | 1.5 µm | 50% of particles, (SRRG Powder) |
Ferro IP 760 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 1.5 µm | 1.5 µm | 50% of particles, (SRRG Powder) |
Ferro IP 780 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 1.5 µm | 1.5 µm | 50% of particles, (SRRG Powder) |
Ferro IP 820 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 1.5 µm | 1.5 µm | 50% of particles, (SRRG Powder) |
Ferro IP 830 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 1.5 µm | 1.5 µm | 50% of particles, (SRRG Powder) |
Ferro IP 900 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Si-Pb-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 1.5 - 2.5 µm | 1.5 - 2.5 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade F Titanium Diboride, TiB2 Powder for sintering.Hot-pressed composites of excellent electrical conductivity, e.g., evaporation boats for continuous aluminum metallizingCrucible material for non-ferrous metalsCeramic shapes to.. |
|||
Particle Size | 1.5 - 3.0 µm | 1.5 - 3.0 µm | Laser Diffraction D50 |
H.C. Starck Grade II Amorphous Boron Automotive (igniter in airbags and belt tighteners)Additive in pyrotechnic mixtures (flares, igniters, and delay compositions)Additive in solid rocket propellant fuels and explosivesPreparation of r.. |
|||
Particle Size | 1.5 µm | 1.5 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade ST Silicon Nitride, Si3N4 Alpha phase > 84%. Standard and cost effective grade.Ceramic cutting toolsHeavy duty components in automotive enginesHigh performance parts for mechanical engineeringBearing components, like high pr.. |
|||
Particle Size | 1.5 µm | 1.5 µm | 50% of particles |
Ferro EG 2992 Glaze and Sealant Glass Glass Type: Bi-Zn-B Typical Powder Form: SRRG Typical Application: Ferrites Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insu.. |
|||
Particle Size | 1.5 µm | 1.5 µm | 50% of particles, (SRRG Powder) |
Ferro IP 730 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 1.5 µm | 1.5 µm | 50% of particles, (SRRG Powder) |
Ferro IP 745 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 1.5 µm | 1.5 µm | 50% of particles, (SRRG Powder) |
Ferro IP 770 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 1.5 - 4.0 µm | 1.5 - 4.0 µm | Laser Diffraction D50 |
H.C. Starck Grade D Titanium Carbonitride Narrow grain distribution and low oxygen contentHard metals (tooling and machining)CermetsBlack ceramics |
|||
Particle Size | 1.5 µm | 1.5 µm | |
Dow Latex LXC 8283NAP Carboxylated Styrene-Butadiene Latex Applications: Latex LXC 8283NAP for carpet is a soft latex with exceptional hand specifically for the rug market.Benefits: Soft handExcellent filler acceptanceGood compatibility with other latexesIn.. |
|||
Particle Size | 1.5 µm | 1.5 µm | @ 10% |
CIMBAR MV 607 Talc MV Series talcs are produced from high purity talc ore, which provide good color, acid resistance and excellent barrier properties when used in paint & coating formulations. MV Series talcs are pla.. |
|||
Particle Size | 1.5 µm | 1.5 µm | D50 |
Dandong Taico Minerals TAICOCITE® TC80 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Particle Size | 1.5 µm | 1.5 µm | @ 10% |
CIMBAR RiverCal™ 8103 & 8103C Calcium Carbonate (CaCO3) RiverCal™ 8100 Series Calcium Carbonate are high purity, white, functional fillers targeted for use in thermosets, thermoplastics, paint & coatings, sealants, TPO's and TPE's and other applications.. |
|||
Particle Size | 1.5 µm | 1.5 µm | @ 10%; Micrometrics Sedigraph 5100 |
CIMBAR RP 9310 Talc RP 9300 Series talcs are produced from high purity ores, which provide an excellent balance of color and mechanical properties, for primary use in commodity polypropylene and polyester compounds. R.. |
|||
Particle Size | 1.5 µm | 1.5 µm | |
Astro Met ZTA 96 Zirconia Toughened Alumina General Description:ZTA-96 is a zirconia toughened alumina ceramic that exhibits excellent wear and corrosion resistance along with high strength and toughness. Astro Met has developed ZTA-96 zircon.. |