Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 10 µm | 10 µm | |
Poco Graphite PLS Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
Particle Size | 10 µm | 10 µm | Median Diameter |
Omya PULPROWHITE® 10 - SA Calcium Carbonate A dry ground calcium carbonate with an intermediate and closely sized particle distribution.Information supplied by Omya North America. |
|||
Particle Size | 10 µm | 10 µm | Mean |
Osprey Metals 410L Stainless Steel Powder (Grade 90% - 22) Particle size distribution 1-250 microns. Typical distribution:90% < 22 microns80% < 16 microns52% < 10 microns15% < 5 micronsMean size is 10.0 microns.SHAPE: Predominantly spherical PACKAGING:.. |
|||
Particle Size | 10 µm | 10 µm | Mean |
Osprey Metals 420/MA Stainless Steel Powder (Grade 90% - 22) Particle size distribution 1-250 microns. Typical distribution:90% < 22 microns80% < 16 microns52% < 10 microns15% < 5 micronsMean size is 10.0 microns.Master alloy blended with 3 parts iron to p.. |
|||
Particle Size | 10 µm | 10 µm | Mean |
Osprey Metals Ni40Cu Binary Alloy Powder (Grade 90% - 22) Particle size distribution 1-250 microns. Typical distribution:90% < 22 microns80% < 16 microns52% < 10 microns15% < 5 micronsMean size is 10.0 microns.SHAPE: Predominantly spherical PACKAGING:.. |
|||
Particle Size | 10 µm | 10 µm | Mean |
Osprey Metals Cu10Al Powder (Grade 90% - 22) Particle size distribution 1-250 microns. Typical distribution:90% < 22 microns80% < 16 microns52% < 10 microns15% < 5 micronsMean size is 10.0 microns.SHAPE: Predominantly spherical PACKAGING:.. |
|||
Particle Size | 10 - 16 µm | 10 - 16 µm | 50% of particles, (TF Powder) |
Ferro CF 7555 Low-Temperature Sealing VITREOUS Typical Powder Form: VSD, TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific .. |
|||
Particle Size | <= 10 µm | <= 10 µm | SRRG Powder |
Ferro EG 0225 Specialty Glass Glass Type: MG-Al-Si (devitrified) Typical Powder Form: MVG, SRRG Typical Application: Sintering Aid / Ceramic Ferro offers a wide range of compositions for specialty applications including sinteri.. |
|||
Particle Size | <= 10 µm | <= 10 µm | 69% finer |
Malvern Minerals Novacite® 1250 Untreated Lamellar Quartz Filler/Extender Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
Particle Size | 10 µm | 10 µm | 87% finer than |
Imerys KT Cast Slurryâ„¢ Kaolin KT Cast Slurry is a carefully controlled kaolin-water suspension formulated for use in ceramic operations.Information provided by Imerys |
|||
Particle Size | 10 µm | 10 µm | 87% finer than |
Imerys KT Castâ„¢ Kaolin KT Cast is a coarse-grained, white firing kaolin that is used primarily in casting bodies based on its fast casting and exceptional deflocculation characteristics.Information provided by Imerys |
|||
Particle Size | 10 µm | 10 µm | 99% finer than |
Imerys Mercapâ„¢ 100 Kaolin Information provided by Imerys |
|||
Particle Size | 10 µm | 10 µm | 30% finer than |
Imerys Minsilsparâ„¢ Feldspar Minsilspar is a 170 mesh feldspathic sand (sandspar) used primarily in the Sanitaryware industry.Information provided by Imerys |
|||
Particle Size | 10 µm | 10 µm | Average Particle Diameter |
Mitsui UNISTOLEâ„¢ R-100S1 Polyolefinic Primer/ Adhesive UNISTOLEâ„¢ R is a modified polyolefin dispersed in hydrocarbon-based solvent used as an adhesive for bonding metals to polyolefins. This can also be used as a metal coating agent. Characteristi.. |
|||
Particle Size | <= 10 µm | <= 10 µm | SRRG Powder |
Ferro IP 770 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 10 µm | 10 µm | 95%, Laser diffraction; QSOP-5&75 |
Shamrock Technologies Fluoro T® 815 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Particle Size | 10 µm | 10 µm | 95%, Laser diffraction; QSOP-5&75 |
Shamrock Technologies MicroFLON® 1253 Thermoplastic Grade PTFE Additive Special grade for fine dispersion.The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a.. |
|||
Particle Size | 10 - 200 µm | 10 - 200 µm | |
SPHERE ONE EXTENDOSPHERESâ„¢ PM 6550 Hollow Plastic Spheres PM 6550 PM 6550 is an extremely light and versatile hollow sphere. Its plastic composition results in a very low density product. Only a very small amount of this hollow sphere is needed to provide .. |
|||
Particle Size | 10 - 15 µm | 10 - 15 µm | |
China Tungsten YG6C Tungsten Carbide Powder Information provided by China Tungsten |
|||
Particle Size | 10 µm | 10 µm | Target Median Particle Size |
CIMBAR Crescent 12 Calcium Carbonate (CaCO3), Fine Powder CIMBAR's Crescent product line is a natural calcium carbonate ground to various particle size distributions. The crystalline structure of the calcium carbonate in Crescent products has a predominan.. |
|||
Particle Size | 10 µm | 10 µm | Median |
CIMBAR BariScan Ultra Chemically Purified White Barium Sulfate (BaSO4) BariScan barite products are produced using a proprietary chemical process to enhance the purity of the natural barium sulfate ore. BariScan and BariScan Ultra barite meet and exceed the requireme.. |
|||
Particle Size | 10 µm | 10 µm | D50 |
CIMBAR MV 610 Talc MV Series talcs are produced from high purity talc ore, which provide good color, acid resistance and excellent barrier properties when used in paint & coating formulations. MV Series talcs are pla.. |
|||
Particle Size | 10 - 16 µm | 10 - 16 µm | D(0.5) |
Akzo Nobel Expancel® 053 WU 40 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 10 - 16 µm | 10 - 16 µm | D(0.5) |
Akzo Nobel Expancel® 820 SLU 40 Unexpanded microspheres in aqueous dispersion Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | <= 10 µm | <= 10 µm | 90% smaller than |
Nyco 10 ES WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 10 - 16 µm | 10 - 16 µm | D(0.5) |
Akzo Nobel Expancel® 642 WU 40 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 10 - 500 µm | 10 - 500 µm | |
Solvay MIRAPOL® SURF-S PFREE POWER Surfactant Description: Blend of acrylic based polymer and sodium carbonate. This polymer is used as a rinse-aid agent to replace the nonionic surfactant 3-in-1 product in automatic dish wash. It is very effic.. |
|||
Particle Size | 10 µm | 10 µm | Mean |
Osprey Metals 310S Stainless Steel Powder (Grade 90% - 22) Particle size distribution 1-250 microns. Typical distribution:90% < 22 microns80% < 16 microns52% < 10 microns15% < 5 micronsMean size is 10.0 microns.SHAPE: Predominantly spherical PACKAGING:.. |
|||
Particle Size | 10 µm | 10 µm | Mean |
Osprey Metals Co452 Cobalt Alloy Powder (Grade 90% - 22) Particle size distribution 1-250 microns. Typical distribution:90% < 22 microns80% < 16 microns52% < 10 microns15% < 5 micronsMean size is 10.0 microns.SHAPE: Predominantly spherical PACKAGING:.. |