Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 12.8 µm | 12.8 µm | d90, Typical |
TIMCAL TIMREX® SFG10 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 12.8 µm | 12.8 µm | d90, Typical |
TIMCAL TIMREX® SFG6 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |