Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 14 µm | 14 µm | median; Microtrac |
Nyco NYGLOS® STPO Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Particle Size | 14 µm | 14 µm | Average Diameter |
Potters Industries Conduct-O-Fil® SH400S33 Silver-Coated Hollow Glass Spheres Conduct-O-Fil® Conductive Particles are engineered to meet a broad range of conductive and electro magnetic interference requirements. Applications include conductive paints and coatings, aerospac.. |
|||
Particle Size | 14 µm | 14 µm | Average Diameter |
Potters Industries Conduct-O-Fil® S5000-S3 Silver-Coated Solid Glass Spheres Conduct-O-Fil® Conductive Particles are engineered to meet a broad range of conductive and electro magnetic interference requirements. Applications include EMI shielding, conductive adhesives, Z-a.. |
|||
Particle Size | 14 µm | 14 µm | mean; 99% -325 mesh |
Momentive Performance Materials HCT-30 Titanium Diboride (TiB2) Powder A high purity powder, grade HCT has virtually no second phase contaminants and only low, controlled levels of carbon, oxygen and nitrogen. Alkalis, alkaline earth, and most metals are typically u.. |
|||
Particle Size | 14 µm | 14 µm | mean; 99% -325 mesh |
Momentive Performance Materials HCT-30D Titanium Diboride (TiB2) Powder Grade HCT-30D is tailored for fabrication by the hot-pressing process. Its composition provides for ease and optimizes the mechanical properties of the component shapes.Titanium Diboride Powder .. |
|||
Particle Size | 14 µm | 14 µm | mean; 99% -325 mesh |
Momentive Performance Materials HCT-40 Titanium Diboride (TiB2) Powder A high purity powder, grade HCT has virtually no second phase contaminants and only low, controlled levels of carbon, oxygen and nitrogen. Alkalis, alkaline earth, and most metals are typically u.. |
|||
Particle Size | 14 - 20 µm | 14 - 20 µm | 10% |
H.C. Starck Amperit® 583.054 Chromium Carbide-Nickel 83-17 (Cr3C2-Ni) |
|||
Particle Size | 14 - 38 µm | 14 - 38 µm | d90 |
Indium Corp. In2O3 Type A Indium Oxide, Crystalline Powder Indium Sesquioxide is a yellow colored powder. It is a stable ceramic-like material, insoluble in water and volatizes at 850°C. Indium sesquioxide is a n-type semiconductor and as such is used .. |
|||
Particle Size | 14 - 19 µm | 14 - 19 µm | 10% |
H.C. Starck Amperit® 553.074 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr) |
|||
Particle Size | 14 - 18 µm | 14 - 18 µm | 50% |
H.C. Starck Amperit® 554.071 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr) |
|||
Particle Size | 14 µm | 14 µm | 95%, Laser diffraction; QSOP-5&75 |
Shamrock Technologies Fluoro T® 811 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline "A" Series A-222FG A-222FG is a fine, non-leafing aluminum pigment with good opacity for solvent based industrial coatings. This grade has a cornflake geometry and wide particle size distribution range. This grade can.. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline 4-Allâ„¢ E2776AR The 4-Allâ„¢ series of passivated aluminum pigments is designed for use in waterborne automotive and industrial coatings. In the 4-Allâ„¢ system, the aluminum pigment is passivated using a pr.. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline Aquasil® "BP" 5500 Silberline has specifically created Aquasil® BP grades for aqueous architectural and industrial maintenance coatings. This family offers a cost-effective alternative for achieving stability and .. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline Aquasil® "BP" SN Silberline has specifically created Aquasil® BP grades for aqueous architectural and industrial maintenance coatings. This family offers a cost-effective alternative for achieving stability and .. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline Aquavet® 5500nl-136M Aquavet® grades are aluminum pigment pellets designed for use in aqueous inks for flexographic and gravure printing. The pellets are composed of 80% aluminum pigment and 20% of a proprietary poly.. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline Lansford 243 Standard Series Lansford 243 - is a fine, non-leafing aluminum pigment with good opacity for solvent based industrial coatings. This is a very economical grade with cornflake geometry and wide particle size distrib.. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline SilBerCote® 5000-20Z SilBerCote® Z polymer treated aluminum pigments are resistant to acid and alkali staining, while providing enhanced electrical charge resistance in finished coatings. Product is typically formula.. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline SilBerCote® 5588-20Y SilBerCote® Y polymer treated aluminum pigments are resistant to acid and alkali staining, while providing enhanced electrical charge resistance in finished coatings. SilBerCote® Y imparts add.. |
|||
Particle Size | 14 µm | 14 µm | Before Conversion |
Silberline Silvet® 320-20-J Silvet® "J" pigments are leafing and non-leafing aluminum pigment pellets designed for ease of handling and incorporation in solvent borne flexographic and gravure ink formulations. The pigment p.. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline Silvex® 223-20-C Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline Silvex® 225-20-D Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Particle Size | 14 - 16 µm | 14 - 16 µm | D50 |
Sinotek Materials ZSG-15 Spherical Graphite Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification.. |
|||
Particle Size | 14 µm | 14 µm | 95%, Laser diffraction; QSOP-5&75 |
Shamrock Technologies Fluoro T® 611 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline Aquavexâ„¢ E5000-AR-207S Aquavexâ„¢ grades are aluminum pigment pellets designed for use in aqueous inks for flexographic and gravure printing. The pellets are composed of 80% aluminum pigment and 20% of a proprietary no.. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline Sparkle Silver® 5000-AR Sparkle Silver® 5000-AR is a fine, bright, non-leafing aluminum pigment with a narrow particle size distribution. It provides exceptional brightness and is acid resistant.Applications: Automotive.. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline Sparkle Silver® 5500 Sparkle Silver® 5500 is a fine, regular purity, non-leafing aluminum pigment. It is characterized by a relatively wide particle size distribution.Applications: Automotive; General Industrial |
|||
Particle Size | 14 µm | 14 µm | |
Silberline Sparkle Silver® Premier 572 Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Particle Size | 14 - 20 µm | 14 - 20 µm | d90, Guaranteed |
TIMCAL TIMREX® C-LUB 306 Primary Synthetic Graphite Information provided by TIMCAL |
|||
Particle Size | 14 µm | 14 µm | Median |
Excalibar ExCal® CW 325 Calcium Carbonate CaCO3 Powder ExCal® CW calcium carbonate products are processed from a high-purity ore, to exacting specifications at the Houston, Texas plant. These grades are processed for use in plastics, rubber, coatings,.. |