Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 10.5 - 14.5 µm | 10.5 - 14.5 µm | d90, Guaranteed |
TIMCAL TIMREX® KS10 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all production.. |