Polymer Property : Particle Size = 145 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 145 µm
145 µm
Average Particle SizeGeon® DFT 1466; Internal Method
PolyOne Geon™ Specialty Suspension Atlas S140 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® Atlas S140 is high molecular weight homopolymer specialty suspension resin intended for use in high strength extruded parts. It improves the physical performance of end application for intsan..
Particle Size 145 µm
145 µm
Springback 20.5%, pressure 0.477 t/cc
TIMCAL TIMREX® KS15 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 145 µm
145 µm
springback 24%, pressure 0.477 t/cc
TIMCAL TIMREX® T150 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 145 µm
145 µm
springback 24%, pressure at 0.477 t/cc
TIMCAL TIMREX® T15-75 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 145 µm
145 µm
at a density of 1.39 g/cc, pressure of 2.5 t/cc
TIMCAL TIMREX® T44 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 145 µm
145 µm
springback 24%, pressure of 0.477 t/cc
TIMCAL TIMREX® T44 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 145 µm
145 µm
springback 24%, pressure at 0.0477t/gg
TIMCAL TIMREX® T75 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..