Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 150 - 250 µm | 150 - 250 µm | Range |
Potters Industries Spheriglass® 1922 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Particle Size | 150 µm | 150 µm | Average Particle SizeGeon® DFT 1466; Internal Method |
PolyOne Geon™ Specialty Suspension Atlas E 43 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Atlas E 43 is a non-chain modified ultra-high molecular weight homopolymer specialty suspension resin intended for use in high strength extruded parts. It improves the physical properties, fo.. |
|||
Particle Size | 150 µm | 150 µm | Average Particle SizeGeon® DFT 1466; Internal Method |
PolyOne Geon™ Specialty Suspension Atlas E 46 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Atlas E 46 is high molecular weight homopolymer specialty suspension resin intended for use in high strength extruded parts. It improves the physical performance of end application for instan.. |
|||
Particle Size | 150 µm | 150 µm | Average Particle SizeGeon® STP 1466; Internal Method |
PolyOne Geon™ Specialty Suspension Impel S100 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Impel S100 is a homopolymer specialty suspension resin intended for use in highly plasticized extrusion and injection molding formulations. It gives superior plasticizer absorption properties.. |
|||
Particle Size | 150 - 210 µm | 150 - 210 µm | |
Potters Industries A-Series P-0080 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Particle Size | <= 150 µm | <= 150 µm | |
Ferro EG 2770 Specialty Glass Glass Type: Si-Al-Mg-Ca Typical Powder Form: TF Typical Application: Sintering Aid Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-ph.. |
|||
Particle Size | >= 150 µm | >= 150 µm | pan, 7% |
ICO Polymers ICOFLOâ„¢ 510-5005 1000 Micron EVA Powder Description: ICOFLO 510-5005 is an EVA powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in masterbatch (inste.. |
|||
Particle Size | >= 150 µm | >= 150 µm | pan, 13% |
ICO Polymers ICOFLOâ„¢ 510-5018 400 Micron LDPE Powder Description: ICOFLO 510-5018 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | >= 150 µm | >= 150 µm | pan, 10% |
ICO Polymers ICOFLOâ„¢ 510-5049 400 Micron LDPE Powder Description: ICOFLO 510-5049 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | >= 150 µm | >= 150 µm | pan, 10% |
ICO Polymers ICOFLOâ„¢ 510-5050 500 Micron LDPE Powder Description: ICOFLO 510-5050 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | >= 150 µm | >= 150 µm | pan, 10% |
ICO Polymers ICOFLOâ„¢ 510-5051 800 Micron LDPE Powder Description: ICOFLO 510-5051 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | >= 150 µm | >= 150 µm | pan, 10% |
ICO Polymers ICOFLOâ„¢ 510-5052 1200 Micron LDPE Powder Description: ICOFLO 510-5052 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in m.. |
|||
Particle Size | >= 150 µm | >= 150 µm | pan, 13% |
ICO Polymers ICOFLOâ„¢ 510-5053 500 Micron LDPE Powder Description: ICOFLO 510-5053 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | >= 150 µm | >= 150 µm | pan, 13% |
ICO Polymers ICOFLOâ„¢ 510-5054 800 Micron LDPE Powder Description: ICOFLO 510-5054 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | >= 150 µm | >= 150 µm | pan, 13% |
ICO Polymers ICOFLOâ„¢ 510-5055 1200 Micron LDPE Powder Description: ICOFLO 510-5055 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | >= 150 µm | >= 150 µm | pan, 13% |
ICO Polymers ICOFLOâ„¢ 510-5059 500 Micron LDPE Powder Description: ICOFLO 510-5059 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | >= 150 µm | >= 150 µm | pan, 13% |
ICO Polymers ICOFLOâ„¢ 510-5061 1200 Micron LDPE Powder Description: ICOFLO 510-5061 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | >= 150 µm | >= 150 µm | pan, 7% |
ICO Polymers ICOTEXâ„¢ 520-5005 1000 Micron EVA Powder Description: ICOTEX 520-5005 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: very high melt flow, fast melting, great .. |
|||
Particle Size | >= 150 µm | >= 150 µm | pan, 13% |
ICO Polymers ICOTEXâ„¢ 520-5059 500 Micron LDPE Powder Description: ICOTEX 520-5059 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Information provided by ICO Polymers.A Sch.. |
|||
Particle Size | >= 150 µm | >= 150 µm | pan, 9% |
ICO Polymers ICOTEXâ„¢ 520-5062 500 Micron LDPE Powder Description: ICOTEX 520-5062 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: very high melt flow, .. |
|||
Particle Size | >= 150 µm | >= 150 µm | pan, 7% |
ICO Polymers ICOTEXâ„¢ 520-5076 500 Micron EVA Powder Description: ICOTEX 520-5076 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Its key characteristics are a good melt flow and flexibility,.. |
|||
Particle Size | <= 150 µm | <= 150 µm | Maximum of .2% greater than |
H.C. Starck Amperit® 205.5 Dense Coated Nickel Graphite 75-25 (Ni-C) |
|||
Particle Size | >= 150 µm | >= 150 µm | pan, 9% |
ICO Polymers ICOFLOâ„¢ 510-5064 1200 Micron LDPE Powder Description: ICOFLO 510-5064 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 150 µm | <= 150 µm | <3% |
Solvay Chemicals Oxyper® S131 Sodium Percarbonate Oxyper® S131 is a stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in bleach additive products and environmental applications; it may be suitabl.. |
|||
Particle Size | <= 150 µm | <= 150 µm | <2% |
Solvay Chemicals Oxyper® S142 Sodium Percarbonate Oxyper® S142 is a stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in formulated bleach additive products, detergent powders and tablets, automa.. |
|||
Particle Size | <= 150 µm | <= 150 µm | <2% |
Solvay Chemicals Oxyper® SHC Sodium Percarbonate Oxyper® SHC is a high coated, stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in bleach additive products, detergent powders and tablets, autom.. |
|||
Particle Size | >= 150 µm | >= 150 µm | d90, 7%, vibrated sieving |
TIMCAL TIMREX® M100 mesh FR Natural Flake Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | <= 150 µm | <= 150 µm | |
TIMCAL TIMREX® M150 mesh FR Natural Flake Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | 150 µm | 150 µm | Average; D50; Laser scattering; ISO 13320-1 |
Braskem UTEC® 3041 Ultra High Molecular Weight Polyethylene Applications which require high impact resistance and use of pigments and/or additives - filters, technical and porous parts, compression molded sheets.Information provided by Braskem. |
|||
Particle Size | 150 - 1200 µm | 150 - 1200 µm | Average value: 404 µm Grade Count:26 |
Overview of materials for Low Density Polyethylene (LDPE), Masterbatch Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Masterbatch Grade". Each property range of values reported is minimum a.. |