Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | >= 2.0 µm | >= 2.0 µm | Primary Crystal Size |
Nabaltec NABALOX® NO 115-25 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | 2.0 µm | 2.0 µm | Median Grain Diameter |
Nabaltec NABALOX® NO 313 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | >= 2.0 µm | >= 2.0 µm | Primary Crystal Size |
Nabaltec NABALOX® NO 615-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | 2.0 µm | 2.0 µm | Median Diameter |
Omya OMYACARB® 520 - FL Calcium Carbonate A high purity, fine, wet ground natural calcium carbonate surface-treated and activated for low humidity content.Applications: Adhesive applications where low moisture content and pick up is require.. |
|||
Particle Size | 2.0 - 4.5 µm | 2.0 - 4.5 µm | Primary crystal size |
Magyar Aluminum ALO-Ex34 Alumina Calcined Alumina |
|||
Particle Size | 2.0 - 5.0 µm | 2.0 - 5.0 µm | d50 |
Magyar Aluminum ALO-G32-2 Alumina Ground Alumina |
|||
Particle Size | 2.0 - 5.0 µm | 2.0 - 5.0 µm | d50 |
Magyar Aluminum ALO-G5-4 Alumina Ground Alumina |
|||
Particle Size | 2.0 - 4.0 µm | 2.0 - 4.0 µm | d50 |
Magyar Aluminum ALO-P95-01 Alumina Alumina for Polishing |
|||
Particle Size | >= 2.0 µm | >= 2.0 µm | 2% finer |
Malvern Minerals Novacite® L-207A Untreated Lamellar Quartz Filler/Extender Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
Particle Size | 2.0 µm | 2.0 µm | 58% finer than |
Imerys Ewingâ„¢ Kaolin Ewing is an intermediate grained air-floated kaolin which is selected, processed and controlled to meet specific requirements of the fibreglass industry.Information provided by Imerys |
|||
Particle Size | 2.0 µm | 2.0 µm | 89% finer than |
Imerys Hamiltonâ„¢ Kaolin Hamilton is a fine-grained kaolin with low alkali content and high PCE. These properties make for ideal air-set refractory mortars. Halloysite content provides excellent suspension and trowel abilit.. |
|||
Particle Size | 2.0 µm | 2.0 µm | 57% finer than |
Imerys Kaolin Slurryâ„¢ Kaolin Slurry is a carefully controlled Kaolin-water suspension formulated for use in cermic castings.Information provided by Imerys |
|||
Particle Size | <= 2.0 µm | <= 2.0 µm | Main Break; Fineness of Grind |
Gwent Electronic Materials C2021031D2 Electrode Ink Electrode Ink C2021031D2 is a Silver Palladium (85/15) electrode ink, designed for use with PVB Tape. It has been specifically formulated for use with PZT ceramics.The ink is in a ready to use form.. |
|||
Particle Size | 2.0 - 5.0 µm | 2.0 - 5.0 µm | Average |
H.C. Starck Grade A Titanium Carbonitride Hard metals (tooling and machining)CermetsBlack ceramics |
|||
Particle Size | 2.0 - 5.0 µm | 2.0 - 5.0 µm | Average |
H.C. Starck Grade A Titanium Nitride Additive for ceramic parts to increase electrical conductivityConstituent for cermets and black ceramicsRaw material for TiN sputter targets |
|||
Particle Size | 2.0 µm | 2.0 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade HD 07 Boron Carbide, B4C Powder for hot-pressing.Abrasive grit or powder (grinding, lapping, polishing)Wear resistant engineering components (e.g. sand-blasting and water jet nozzlesLight weight ceramic armorMetal infiltrat.. |
|||
Particle Size | 2.0 - 3.0 µm | 2.0 - 3.0 µm | Average |
H.C. Starck High Vacuum 250 Titanium Carbide, TiC Hard metals (tooling and machining)CementsBlack ceramics, e.g. (Al2O3-TiC) |
|||
Particle Size | 2.0 - 3.0 µm | 2.0 - 3.0 µm | Average |
H.C. Starck Standard 250 Titanium Carbide, TiC Hard metals (tooling and machining)CementsBlack ceramics, e.g. (Al2O3-TiC) |
|||
Particle Size | 2.0 - 4.5 µm | 2.0 - 4.5 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade B Aluminum Nitride AIN High thermally conductive ceramicsComposite ceramicsSiAlONsHeat sinksElectrically insulating packages for electronicsCrucibles for metals and salt meltsThermally conductive filler for polymersCompon.. |
|||
Particle Size | 2.0 - 3.0 µm | 2.0 - 3.0 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade C Molybdenum Disilicide MoSi2 Composite ceramicsHeating elementsConstituent of glow plugs for enginesRaw material for MoSi2 sputter target (PVD) |
|||
Particle Size | 2.0 - 5.0 µm | 2.0 - 5.0 µm | D 50%; Laser Light Diffraction per ASTM C1070 |
H.C. Starck Type II Pure Molybdenum MIMP Powder Description of Product: Highly deagglomerated high purity molybdenum powder for any applications requiring the most finely deagglomerated powders like paste or metal injection molding applications... |
|||
Particle Size | 2.0 µm | 2.0 µm | |
Shin-Etsu Silicones KM-9729 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Particle Size | 2.0 - 50 µm | 2.0 - 50 µm | PSD (d<sub>50</sub> |
Terio Corporation TZOH-50 Zirconium Hydroxide Information provided by TERIO Corporation. |
|||
Particle Size | 2.0 µm | 2.0 µm | Median Grain (d50) |
CeramTec Rubalit® 710 Alumina, 99.6% Rubalit® 710 (99.6%) is an alumina that produces optimum results and is considered the material of choice for thin-film technology. Its characterizing features are high strength and thermal conduct.. |
|||
Particle Size | 2.0 - 10 µm | 2.0 - 10 µm | |
American Elements Silver Nanoparticles General DescriptionSilver (Ag) Nanoparticles, nanodots or nanopowder are spherical or flake high surface area metal particles. Nanoscale Silver Particles are typically 1 - 40 nanometers (nm) with sp.. |
|||
Particle Size | 2.0 - 7.0 µm | 2.0 - 7.0 µm | |
Dow Corning EP-9215 Cosmetic Powder A hard white elastomeric silicone powder that provides a silky and powdery skin feel, along with oil and sebum absorption. It also improves color intensity and coverage in pressed powder formulation.. |
|||
Particle Size | 2.0 µm | 2.0 µm | Average Crystal Size - Thin Section Test |
CoorsTek Tungsten Carbide, WC Information provided by CoorsTek. |
|||
Particle Size | 2.0 µm | 2.0 µm | Hegman; Grinde Gauge |
3M Dyneon™ J14 PTFE Micropowder 3M™ Dyneon™ PTFE Micropowders can be used as additives in many applications and at concentrations typically from 5 to 20%. Homogeneous incorporation is the single most important process and applic.. |
|||
Particle Size | <= 2.0 µm | <= 2.0 µm | 10% |
BYK Cloisite® 30B Nanoclay Cloisite® 30B is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.
Information provided by Southern Clay ProductsSouthern Clay P.. |