Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 2.8 µm | 2.8 µm | d10 |
TIMCAL TIMREX® HSAG100 Primary Synthetic High Surface Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 2.8 µm | 2.8 µm | |
Dow Everest™ 200 Latex Modified Acrylic Emulsion Applications:EVEREST 200 is based on a unique modified acrylic technology, that was developed to address the growing interest in carpet backing technologies with sustainable attributes. This high so.. |