Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 4.0 µm | 4.0 µm | median; Microtrac |
Nyco M1250 AS WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Particle Size | 4.0 µm | 4.0 µm | median; Microtrac |
Nyco M1250 ES WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 4.0 µm | 4.0 µm | median; Microtrac |
Nyco M1250 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Particle Size | >= 4.0 µm | >= 4.0 µm | 10% smaller than |
Nyco M200 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 4.0 µm | 4.0 µm | median; Microtrac |
Nyco MD1250 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | >= 4.0 µm | >= 4.0 µm | 10% smaller than |
Nyco NYAD® MD200 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | >= 4.0 µm | >= 4.0 µm | 10% smaller than |
Nyco NYGLOS® 8 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Particle Size | 4.0 µm | 4.0 µm | Average Diameter |
Potters Industries Conduct-O-Fil® SC04P10 Silver-coated Sub-10 micron Particles Applications include conductive inks, conductive adhesives, partial replacement of pure silver powder. Features good conductivity, possible blends/ replacement of 100% pure silver, silver/glass has.. |
|||
Particle Size | 4.0 µm | 4.0 µm | |
Poco Graphite DFP-3-2 Ion Implant Grade Graphite This is a high strength graphite that has reduced porosity. DFP-3-2 has long been the standard for components that exhibit long life and reduced erosion rates. |
|||
Particle Size | <= 4.0 µm | <= 4.0 µm | |
Poco Graphite EDM-4 EDM Graphite POCO's EDM-4 is our premier offering in the Ultrafine classification. This highly isotropic grade combines strength with moderate hardness, yielding superior electrode fabrication characteristics. T.. |
|||
Particle Size | 4.0 µm | 4.0 µm | 50% of particles, (RWG Powder) |
Ferro IX 2443 Passivation Glasses - High Voltage (Zn-B-Silicates) Typical Powder Form: RWG, DSD Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures a.. |
|||
Particle Size | 4.0 - 7.0 µm | 4.0 - 7.0 µm | d90 |
Magyar Aluminum ALO-DN-2S Alumina Reactive Alumina |
|||
Particle Size | 4.0 - 7.0 µm | 4.0 - 7.0 µm | d90 |
Magyar Aluminum ALO-EL-2S Alumina Reactive Alumina |
|||
Particle Size | 4.0 µm | 4.0 µm | d50 |
Magyar Aluminum ALOLT 704 Aluminum Hydroxide Viscosity Optimized Type |
|||
Particle Size | 4.0 - 8.0 µm | 4.0 - 8.0 µm | d50 |
Magyar Aluminum ALO-P90-06 Alumina Alumina for Polishing |
|||
Particle Size | 4.0 µm | 4.0 µm | average |
Inhance Fluoro-Seal INHANCE® Si-8900 Polymer Alloy Product Description: INHANCE S i-8000 series polymer alloy consists of black, medium density, silicon carbide chemically modified for greater adhesion. This product was designed for alloying with v.. |
|||
Particle Size | <= 4.0 µm | <= 4.0 µm | Main Break; Fineness of Grind |
Gwent Electronic Materials C2000808D2 Silver Backlight Ink Silver Ink C2000808D2 is a high resistance ink designed for use as the heating bars and tracks on automobile backlights and other circuits on glass. It has dark color when printed and fired on floa.. |
|||
Particle Size | <= 4.0 µm | <= 4.0 µm | D90 |
Momentive Performance Materials AC6111 Boron Nitride (BN) Powder Agglomeration of submicron hexagonal turbostatic crystals. Used in paints, refractory coatings, mold/die release agents, nucleation aid, and lubricants. It is relatively non-wetting versus molten .. |
|||
Particle Size | <= 4.0 µm | <= 4.0 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade A Yttrium Oxide Sintering additive for Si3N4 and AlNStabilizer for zirconias (PSZ) and insulating coatings (TBC`s)Catalyst carrierYttria stabilized zirconias electrolytes for solid oxide fuel cellsLuminescent mater.. |
|||
Particle Size | <= 4.0 µm | <= 4.0 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade AT Yttrium Oxide Sintering additive for Si3N4 and ALNStabilizer for zirconias (PSZ) and insulating coatings (TBC`s)Catalyst carrierYttria stabilized zirconias electrolytes for solid oxide fuel cellsLuminescent mater.. |
|||
Particle Size | 4.0 µm | 4.0 µm | |
Shin-Etsu Silicones X-52-7042 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Particle Size | 4.0 - 5.0 µm | 4.0 - 5.0 µm | Median Grain (d50) |
CeramTec Alunit® Aluminum Nitride Alunit® offers an extremely high thermal conductivity of 180 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. Its .. |
|||
Particle Size | 4.0 µm | 4.0 µm | D50 (Malvern) Size E |
Vesta Ceramics SicoMill® Grade 2 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Particle Size | 4.0 µm | 4.0 µm | Median |
Excalibar ExBar™ W 4 Barite BaSO4 Powder ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, .. |
|||
Particle Size | 4.0 µm | 4.0 µm | D50 |
Dandong Taico Minerals TAICOCITE® TC12 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Particle Size | 4.0 µm | 4.0 µm | Median |
CIMBAR EliteTalc® 22 Cosmetic Talc Cimbar performance Minerals MV, LLC Talc U.S.P. Cosmetic talcs are designed specifically for cosmetic formulations. Talc is commonly used in cosmetics for its ability to bind to oils, create a mois.. |
|||
Particle Size | 4.0 - 6.0 µm | 4.0 - 6.0 µm | Mean particle size |
Carborundum CarboTherm™ CTUF Boron Nitride Powder Boron Nitride powders have high thermal conductivity, low dielectric loss, and low thermal expansion. They are non-abrading to electronic components, lubricious, non-toxic, and retain their dielect.. |
|||
Particle Size | 4.0 µm | 4.0 µm | 50" Percentile |
3M W-410 Ceramic Microspheres 3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler l.. |
|||
Particle Size | 4.0 - 5.0 µm | 4.0 - 5.0 µm | Medium Grain (d50) |
CeramTec CeramCool® Alunit® Aluminum Nitride CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit.. |