Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | <= 40 µm | <= 40 µm | 90% smaller than |
Nyco NYGLOS® 8 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Particle Size | >= 40 µm | >= 40 µm | 10% smaller than |
Nyco NYGLOS® M50 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | <= 40 µm | <= 40 µm | 90% smaller than |
Nyco NYGLOS® STPO Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Particle Size | <= 40 µm | <= 40 µm | 90% smaller than |
Nyco RRIMGLOS® II Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Particle Size | 40 - 50 µm | 40 - 50 µm | Average; for inner type spray system; Microtrac HRA |
NYC YT3WBHQ Y2O3 Powder for Spray Coating High purity granules produced in clean environment. Uses include semiconductor / LCD industries and electroceramics.Narrow particle size distributionTailorable for each spray coating technologyNo c.. |
|||
Particle Size | 40 µm | 40 µm | |
Silberline Sparkle Silver® 3624 Sparkle Silver® 3624 is a coarse, brilliant, regular purity, non-leafing aluminum pigment popular for solvent-based general industrial coatings. This pigment can be used with tints to produce a w.. |
|||
Particle Size | >= 40 µm | >= 40 µm | 250 Mesh; PS-1-2 |
Solvay JAGUAR® HP 8FF Surfactant Description: Hydroxypropyl guar with extremely low residue, designed to be easily dispersed into water where it will wet out and hydrate, forming a viscous HPG fluid which will readily crosslink wit.. |
|||
Particle Size | 40 - 51.5 µm | 40 - 51.5 µm | d90, Guaranteed |
TIMCAL TIMREX® KS44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 40 - 55 µm | 40 - 55 µm | d90, Guaranteed |
TIMCAL TIMREX® LSG 44 Natural Graphite Flakes TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | 40 µm | 40 µm | D50 (Malvern) Size B |
Vesta Ceramics SicoMill® Grade 2 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Particle Size | <= 40 µm | <= 40 µm | Max |
CIMBAR Miti-Wite B10 Chemically Purified White Barite (BaSO4) Miti-Wite barite products are produced using a proprietary chemical process to enhance the purity of the natural barium sulfate ore. Miti-Wite products are available in a variety of particle sizes .. |
|||
Particle Size | <= 40 µm | <= 40 µm | Max |
CIMBAR BariScan Ultra Chemically Purified White Barium Sulfate (BaSO4) BariScan barite products are produced using a proprietary chemical process to enhance the purity of the natural barium sulfate ore. BariScan and BariScan Ultra barite meet and exceed the requireme.. |
|||
Particle Size | <= 40 µm | <= 40 µm | Max |
CIMBAR CIMBAR™ 325 Barite Powder (BaSO4) CIMBAR barite products are made using only the highest quality white, natural barium sulfate ore. CIMBAR barites unique properties of fine grind, high specific gravity, low solubility and chemical .. |
|||
Particle Size | 40 µm | 40 µm | Average |
Azoty Tarnow™ TARFLEN SM-B30 PTFE Reinforced with 30% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Particle Size | 40 µm | 40 µm | Average |
Azoty Tarnow™ TARFLEN SM-B40 PTFE Reinforced with 40% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Particle Size | 40 µm | 40 µm | Average |
Azoty Tarnow™ TARFLEN SM-G15 PTFE Tarflen SM1 reinforced with 15% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Particle Size | 40 µm | 40 µm | Average |
Azoty Tarnow™ TARFLEN SM-G20 PTFE Reinforced with 20% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Particle Size | 40 µm | 40 µm | Average |
Azoty Tarnow™ TARFLEN SM-S15 PTFE 15% glass fiber reinforced for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Particle Size | 40 µm | 40 µm | Average |
Azoty Tarnow™ TARFLEN SM-S25 PTFE Tarflen SM1 reinforced with 25% glass fiber for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Particle Size | 40 µm | 40 µm | 50th% |
3M S32 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 40 µm | 40 µm | 50th% |
3M S38 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 40 µm | 40 µm | D50 |
3M S38XHS Glass Bubbles 3M™ Glass Bubbles S38XHS have a density of .38 g/cc and an isostatic crush strength of 5500 psi with a minimum survival of 90% as compared to S38HS, which has a target 90% survival of 5500 psi. Lik.. |
|||
Particle Size | 40 - 49 µm | 40 - 49 µm | D50, Range |
3M S38XHS Glass Bubbles 3M™ Glass Bubbles S38XHS have a density of .38 g/cc and an isostatic crush strength of 5500 psi with a minimum survival of 90% as compared to S38HS, which has a target 90% survival of 5500 psi. Lik.. |
|||
Particle Size | 40 µm | 40 µm | 95" Percentile |
3M W-610 Ceramic Microspheres 3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler l.. |
|||
Particle Size | <= 40 µm | <= 40 µm | 90% smaller than |
Nyco ULTRAFIBRE® II Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 40 µm | 40 µm | 50th% |
3M D32/4500 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 40 µm | 40 µm | Average Diameter |
Potters Industries Conduct-O-Fil® SA300S30 Silver-coated Aluminum Granules Applications:EMI shielding in contact with aluminumConductive adhesivesAerospace and marine applicationsAdvantages:Low density with high conductivityLow galvanic corrosion in contact with aluminumIn.. |
|||
Particle Size | 40 µm | 40 µm | Average Diameter |
Potters Industries Conduct-O-Fil® SM40P20 Silver-coated Magnetic Particles Applications:EMI shieldingConductive adhesivesZ-axis conductive filmsAdvantages:Alternative to nickel when neededParticles can be magnetically alignedHalf the density of silver-coated nickelInformat.. |
|||
Particle Size | 40 µm | 40 µm | Average |
Azoty Tarnow™ TARFLEN SM-B60 PTFE Tarflen SM1 reinforced with 60% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Particle Size | 40 µm | 40 µm | Average |
Azoty Tarnow™ TARFLEN SM-K22G3 PTFE Tarflen SM1 reinforced with 22% coke and 3% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |