Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 43 - 57 µm
43 - 57 µm
90%
H.C. Starck Amperit® 582.072 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr)
Particle Size 43 µm
43 µm
d90
TIMCAL TIMREX® HSAG100 Primary Synthetic High Surface Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 43 µm
43 µm
Springback 20.5%, pressure 0.477 t/cc
TIMCAL TIMREX® KS15 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 43 µm
43 µm
Typical
TIMCAL TIMREX® LSG 44 Natural Graphite Flakes
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-..
Particle Size 43 µm
43 µm
springback 20.5%, pressure 0.477 t/cc
TIMCAL TIMREX® T150 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 43 µm
43 µm
springback 20.5%, pressure at 0.477 t/cc
TIMCAL TIMREX® T15-75 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 43 µm
43 µm
springback 20.5%, pressure of 0.477 t/cc
TIMCAL TIMREX® T44 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 43 µm
43 µm
springback 20.5%, pressure at 0.0477t/gg
TIMCAL TIMREX® T75 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 43 µm
43 µm
d90, Typical
TIMCAL TIMREX® C-LUB 310 Primary Synthetic Graphite
Information provided by TIMCAL