Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 5.0 µm | 5.0 µm | |
Poco Graphite AXF-5QC Specialty Graphite, Copper Impregnated SSH hardness is 67.General Poco Specialty Graphite Information: Poco's high strength, fine-grained, isotropic graphites offer maximum design flexibility. Easily machined. High strength and small p.. |
|||
Particle Size | 5.0 µm | 5.0 µm | |
Poco Graphite AXZ-5Q Industrial Grade Graphite POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr.. |
|||
Particle Size | 5.0 µm | 5.0 µm | 72.3% of particles less than |
Old Hickory M&M Clays, Inc. Wilco-LPC Kaolin Clay Wilco LPC is the same selection as the SLU grade except it is in natural shredded or Airfloat (powdered) form. It offers the same benefits in a ceramic casting formulation discussed above for the SL.. |
|||
Particle Size | 5.0 - 150 µm | 5.0 - 150 µm | |
Potters Industries Q-Cel® 5032S Hollow Engineered Glass Microspheres Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me.. |
|||
Particle Size | 5.0 - 150 µm | 5.0 - 150 µm | |
Potters Industries Q-Cel® 7019 Hollow Engineered Glass Microspheres Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me.. |
|||
Particle Size | 5.0 µm | 5.0 µm | 50% of particles |
Ferro EG 0026 Glaze and Sealant Glass Glass Type: Ca-B-Al-Si Typical Powder Form: MVG Typical Application: Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insul.. |
|||
Particle Size | 5.0 µm | 5.0 µm | 50% of particles |
Ferro EG 2705 Glaze and Sealant Glass Glass Type: Ca-Al-Si Typical Powder Form: MVG Typical Application: Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insulat.. |
|||
Particle Size | 5.0 µm | 5.0 µm | 50% of particles |
Ferro EG 2739 Thick Film Glass Glass Type: Pb-Zn-B Typical Powder Form: MVG Typical Application: Resistor Overglaze Ferro produces standard and custom glass products that are used in thick film compositions including resistors, .. |
|||
Particle Size | 5.0 µm | 5.0 µm | 50% of particles, (MVG Powder) |
Ferro IX 2218 Passivation Glasses - High Voltage (Zn-B-Silicates) Typical Powder Form: REG, MVG Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures a.. |
|||
Particle Size | 5.0 - 10 µm | 5.0 - 10 µm | d50 |
Magyar Aluminum ALO-P95-08 Alumina Alumina for Polishing |
|||
Particle Size | 5.0 µm | 5.0 µm | 83% finer than |
Imerys Diamondâ„¢ Kaolin Diamond is an intermediate-grained montmorillonitc kaolin used primarily in plastic formed bodies. This kaolin is known for its good strength and white-firing characteristics.Information provided by.. |
|||
Particle Size | 5.0 µm | 5.0 µm | 79% finer than |
Imerys Ewingâ„¢ Kaolin Ewing is an intermediate grained air-floated kaolin which is selected, processed and controlled to meet specific requirements of the fibreglass industry.Information provided by Imerys |
|||
Particle Size | <= 5.0 µm | <= 5.0 µm | Fineness of Grind |
Gwent Electronic Materials C2030325D14 Curable Carbon Ink This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive coating that combines good adhesion with excellent chemical, solvent and .. |
|||
Particle Size | 5.0 µm | 5.0 µm | 50% of particles |
Ferro EG 2791 Thick Film Glass Glass Type: Bi-Pb-Zn Typical Powder Form: MVG Typical Application: End Termination Ferro produces standard and custom glass products that are used in thick film compositions including resistors, co.. |
|||
Particle Size | <= 5.0 µm | <= 5.0 µm | Main Break; Fineness of Grind |
Gwent Electronic Materials C2031105D2 Palladium Ink Palladium Ink C2031105D2 is an ink formulated for screen printing for use on Fuel Cells. It is suitable for application onto Solid Oxide Fuel Cells.The ink has been made at a ready to use viscosity.. |
|||
Particle Size | 5.0 µm | 5.0 µm | Mean Value, Laser diffraction; QSOP-5&75 |
Shamrock Technologies MicroFLON® 1253 Thermoplastic Grade PTFE Additive Special grade for fine dispersion.The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a.. |
|||
Particle Size | 5.0 µm | 5.0 µm | Springback 9.5%, pressure 0.477 t/cc |
TIMCAL TIMREX® GB99/6 Natural Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | 5.0 µm | 5.0 µm | Springback 11.5%, pressure 0.477 t/cc |
TIMCAL TIMREX® KS150 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 5.0 µm | 5.0 µm | at a density of 1.81 g/cc, pressure at 2.5 t/cc |
TIMCAL TIMREX® KS5-25 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 5.0 µm | 5.0 µm | Springback 8%, pressure 0.477 t/cc |
TIMCAL TIMREX® SFG44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 5.0 µm | 5.0 µm | at a density of 1.90 g/cc, pressure 2.5 t/cc |
TIMCAL TIMREX® SFG75 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 5.0 µm | 5.0 µm | Springback 8%, pressure 0.477 t/cc |
TIMCAL TIMREX® SFG15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 5.0 - 355 µm | 5.0 - 355 µm | |
Trelleborg Fillite® 300W Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Particle Size | 5.0 - 500 µm | 5.0 - 500 µm | |
Trelleborg Fillite® SG (500) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Particle Size | 5.0 µm | 5.0 µm | @ 10% |
CIMBAR RP 9405 Talc RP 9400 Series talcs are produced from ores, which provide an excellent balance of mechanical properties at an economical price, for primary use in commodity polypropylene. RP 9400 Series talcs are.. |
|||
Particle Size | 5.0 - 10 µm | 5.0 - 10 µm | Mean particle size |
Carborundum CarboTherm™ CTF5 Boron Nitride Powder Boron Nitride powders have high thermal conductivity, low dielectric loss, and low thermal expansion. They are non-abrading to electronic components, lubricious, non-toxic, and retain their dielect.. |
|||
Particle Size | 5.0 µm | 5.0 µm | Loosely agglomerated |
Arkema Group KYNAR® LBG1 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder.Applications: Membrane, Lithium ion battery applicationsInformation provided by Arkema Inc. |
|||
Particle Size | >= 5.0 µm | >= 5.0 µm | 10% smaller than |
Nyco ULTRAFIBRE® II Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 5.0 - 355 µm | 5.0 - 355 µm | |
Trelleborg Fillite® PG (300LF) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Particle Size | 5.0 µm | 5.0 µm | Loosely agglomerated |
Arkema Group KYNAR® 2801-00 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasi.. |