Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 500 µm | 500 µm | ASTM D4895 |
3M Dyneon™ TFM™ 2001 Modified PTFE Paste Extrusion Powder
(discontinued **) Type I, gr. 2 PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 1000. Average particle size 500µm.Modified PTFE fine powder product for paste extrusion applications. The modified .. |
|||
Particle Size | 500 µm | 500 µm | average; ISO 12086 |
3M Dyneon™ TF 2053 PTFE
(discontinued **) Processed by standard paste extrusion methodRecommended grade for extrusion of tubing and cables requiring only moderately high reduction ratioGood overall balance of mechanical properties and proce.. |
|||
Particle Size | 500 µm | 500 µm | average; ASTM D4895 |
3M Dyneon™ TF 2071 PTFE
(discontinued **) Processable by standard paste extrusion methodTF 2071 and TF 2072 have a wide processing range because of high maximum allowable reduction ratioTF 2071 is recommended for high quality tubing and wir.. |
|||
Particle Size | 500 µm | 500 µm | average; ISO 12086 |
3M Dyneon™ TFM™ 2001 PTFE
(discontinued **) Processable by standard paste extrusion methodRecommended for high performance applications with reduction ratios up to 1000:1Provides denser polymer structure with fewer micro voids and lower gas p.. |
|||
Particle Size | <= 500 µm | <= 500 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5056 500 Micron LDPE Powder Description: ICOFLO 510-5056 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 500 µm | <= 500 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5062 500 Micron LDPE Powder Description: ICOFLO 510-5062 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 500 µm | <= 500 µm | sieve < 5% |
ICO Polymers ICOTEXâ„¢ 520-5050 500 Micron LDPE Powder Description: ICOTEX 520-5050 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and fa.. |
|||
Particle Size | <= 500 µm | <= 500 µm | sieve < 5% |
ICO Polymers ICOTEXâ„¢ 520-5062 500 Micron LDPE Powder Description: ICOTEX 520-5062 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: very high melt flow, .. |
|||
Particle Size | <= 500 µm | <= 500 µm | sieve < 5% |
ICO Polymers ICOTEXâ„¢ 520-5076 500 Micron EVA Powder Description: ICOTEX 520-5076 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Its key characteristics are a good melt flow and flexibility,.. |
|||
Particle Size | <= 500 µm | <= 500 µm | Grain Size |
Gouda Vuurvast ADHESIET 150 Dry Air-Setting Refractory Mortar Description: Adhesiet 150 is an air setting mortar with a sodium silicate bond and is supplied as a dry powder. Because of the special mix of the raw materials it can be used up to 1500°C.Remarks.. |
|||
Particle Size | <= 500 µm | <= 500 µm | Grain Size |
Gouda Vuurvast ADHESIET 170 P Al Dry Air-Setting Refractory Mortar Description: Adhesiet 170 P Al is a phosphate bonded air setting mortar, supplied as a dry powder. Because of the special choice of raw materials this mortar is especially applied in aluminum meltin.. |
|||
Particle Size | <= 500 µm | <= 500 µm | Grain Size |
Gouda Vuurvast ADHESIET 180 P Dry Air-Setting Refractory Mortar Description: Adhesiet 180 P is a phosphate bonded air setting mortar, supplied as a dry powder. This very pure mortar is for use up to extreme high temperatures.Remarks: Adhesiet mortars can be stor.. |
|||
Particle Size | <= 500 µm | <= 500 µm | Grain Size |
Gouda Vuurvast ADHESIET 180 PCr Dry Air-Setting Refractory Mortar Description: Adhesiet 180 PCr is a Cr2O3 doped corundum mortar with a phosphate bond, supplied as a dry powder. This material is especially developed for high chemical resistance at very high temper.. |
|||
Particle Size | <= 500 µm | <= 500 µm | Grain Size |
Gouda Vuurvast ADHESIET A Dry Air-Setting Refractory Mortar Description: Adhesiet A is a general purpose air setting mortar, supplied as a dry powder for use up to 1400°C.Remarks: Adhesiet mortars can be stored for an unlimited time if kept dry and cool. .. |
|||
Particle Size | 500 - 5000 µm | 500 - 5000 µm | |
Minelco Chilcon Low grade FeSi Hard, wear resistant. Applications: Heavy aggregates, hard wearing floors |
|||
Particle Size | 500 µm | 500 µm | ASTM D 1921 |
Lucobit Lucofin® 1400MN Powder Ethylene Butyl Acrylate Lucofin 1400MN Powder is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400MN Powder is softer and more flexible ethane et.. |
|||
Particle Size | <= 500 µm | <= 500 µm | |
Shandong Dongyue Polymer DF-21B PTFE Presintered Resin Usage: The presintered resin is suitable for continuously extruding of all types, pushing and pressing PTFE rod, tube and special shape.Packing: PTFE is packed in double layer PVC bags inside and in.. |
|||
Particle Size | 500 - 700 µm | 500 - 700 µm | |
Shandong Dongyue Polymer DF-31A PTFE Pelletized Resin Usage: The resin is used to auto press molding and ram extrusion all kinds of rods, pipe etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTF.. |
|||
Particle Size | 500 - 1000 µm | 500 - 1000 µm | 50% Min; 540MA3C5E |
Solvay MIRAPOL® SURF-S 410 Surfactant Description: Granulated rinse aid polymer for use in automatic dish washing powders or tablets. 18% activeIdentification: BLEND OF ACRYLIC BASED POLYMER AND SODIUM TRIPOLYPHOSPHATE.Use level : 0.5 â.. |
|||
Particle Size | 500 µm | 500 µm | |
Daikin POLYFLON F-104 PTFE Fine Powder Processing Methods: Paste extrusion, calendering.Applications: Unsintered tape, sealing tape, low specific gravity tape, tape for wrapping flat cables, tubes.Information provided by Daikin Industrie.. |
|||
Particle Size | 500 µm | 500 µm | |
Daikin POLYFLON F-201 PTFE Fine Powder Processing Methods: Paste extrusion.Applications: Spaghetti tubes, small diameter tubes, fine electric wire smaller than AGW16.Information provided by Daikin Industries. |
|||
Particle Size | 500 µm | 500 µm | |
Daikin POLYFLON F-205 PTFE Fine Powder Processing Methods: Paste extrusion.Applications: Spaghetti tubes, small diameter tubes, fine electric wire smaller than AGW16.Information provided by Daikin Industries. |
|||
Particle Size | 500 µm | 500 µm | ASTM D4894 |
Daikin POLYFLON M-393 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding, automatic compression molding, and ram extrusion.Features: Maximum emphasis given to ease of handling during molding. Used when molded arti.. |
|||
Particle Size | 500 - 850 µm | 500 - 850 µm | min 92%; BC HSZ 326:2001/1 screening |
BorsodChem ONGROSTYR F-I Expandable Polystyrene (EPS) ONGROSTYR F-I is an expandable, flame-retardant styrene homopolymer, produced by suspension polymerization. The product meets the requirements of DIN 4102 and of B1 class of building materials, i.e... |
|||
Particle Size | 500 µm | 500 µm | |
Asahi Glass Fluon® CD090 PTFE Coagulated Dispersion Powder Fluon®PTFE coagulated dispersion powders (fine powders) are used for paste extrusion to make tapes, tubes, rods and wire coatings.Information provided by Asahi Glass Company, Inc. |
|||
Particle Size | 500 µm | 500 µm | average; ISO 13320 |
3M Dyneon™ TF 2021Z PTFE Fine Powder Dyneon TF 2021 Z PTFE is an ideal grade for pipe liner applications because of its outstanding green strength. It is the preferred grade for unsintered thread sealing tapes, expanded join sealings, .. |
|||
Particle Size | 500 µm | 500 µm | VW-10300P; D90 Particle sizes by sieve measurement |
Solvay Specialty Polymers Virantage® VW-10300 P, FP Polyethersulfone (PESU)
(Unverified Data**) Virantage® VW-10300 polyethersulfone (PESU) is a non-functionalized, high-temperature sulfone polymer powder. Two grades are offered: Virantage VW-10300P and Virantage VW-10300FP, providing two par.. |
|||
Particle Size | 500 µm | 500 µm | VW-10700RP; D90 Particle sizes by sieve measurement |
Solvay Specialty Polymers Virantage® VW-10700 RP, RFP, RSFP Polyethersulfone (PESU)
(Unverified Data**)&l Virantage® VW-series functionalized polyethersulfones (r-PESU) are amorphous, high-temperature sulfone polymers featuring reactive end groups to enhance solubility and improve interfacial propertie.. |
|||
Particle Size | <= 500 µm | <= 500 µm | Grain Size |
Gouda Vuurvast ADHESIET 170 P Dry Air-Setting Refractory Mortar Description: Adhesiet 170 P is a phosphate bonded air setting mortar, supplied as a dry powder. Because of the special choice of raw materials this mortar is especially applied in aluminum melting a.. |