Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 500 - 710 µm | 500 - 710 µm | |
Potters Industries A-Series P-0280 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Particle Size | 500 µm | 500 µm | ASTM D4895 |
3M Dyneon™ TFM™ 2001 Modified PTFE Paste Extrusion Powder
(discontinued **) Type I, gr. 2 PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 1000. Average particle size 500µm.Modified PTFE fine powder product for paste extrusion applications. The modified .. |
|||
Particle Size | 500 µm | 500 µm | average; ISO 12086 |
3M Dyneon™ TF 2021 PTFE
(discontinued **) Processable by standard paste extrusion methodsBoth grades can be processed at low to medium reduction ratiosTF 2021 PTFE is preferred for unsintered thread sealing tapes and expanded joint sealants.. |
|||
Particle Size | 500 µm | 500 µm | average; ASTM D4895 |
3M Dyneon™ TF 2025 PTFE
(discontinued **) Processable by standard paste extrusion methodsBoth grades can be processed at low to medium reduction ratiosTF 2021 PTFE is preferred for unsintered thread sealing tapes and expanded joint sealants.. |
|||
Particle Size | 500 µm | 500 µm | average; ISO 12086 |
3M Dyneon™ TF 2029 PTFE
(discontinued **) Processable by standard paste extrusion methodsDesigned for low reduction ratiosCan be processed at a high stretch ratiosRecommended for apes requiring high mechanical strength, such as electrical t.. |
|||
Particle Size | 500 µm | 500 µm | average; ISO 12086 |
3M Dyneon™ TF 2053 PTFE
(discontinued **) Processed by standard paste extrusion methodRecommended grade for extrusion of tubing and cables requiring only moderately high reduction ratioGood overall balance of mechanical properties and proce.. |
|||
Particle Size | 500 µm | 500 µm | average; ASTM D4895 |
3M Dyneon™ TF 2071 PTFE
(discontinued **) Processable by standard paste extrusion methodTF 2071 and TF 2072 have a wide processing range because of high maximum allowable reduction ratioTF 2071 is recommended for high quality tubing and wir.. |
|||
Particle Size | <= 500 µm | <= 500 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5053 500 Micron LDPE Powder Description: ICOFLO 510-5053 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 500 µm | <= 500 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5059 500 Micron LDPE Powder Description: ICOFLO 510-5059 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 500 µm | <= 500 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5062 500 Micron LDPE Powder Description: ICOFLO 510-5062 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 500 µm | <= 500 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5073 500 Micron LLDPE Powder Description: ICOFLO 510-5073 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 500 µm | <= 500 µm | sieve < 5% |
ICO Polymers ICOTEXâ„¢ 520-5076 500 Micron EVA Powder Description: ICOTEX 520-5076 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Its key characteristics are a good melt flow and flexibility,.. |
|||
Particle Size | <= 500 µm | <= 500 µm | Grain Size |
Gouda Vuurvast ADHESIET 150 Dry Air-Setting Refractory Mortar Description: Adhesiet 150 is an air setting mortar with a sodium silicate bond and is supplied as a dry powder. Because of the special mix of the raw materials it can be used up to 1500°C.Remarks.. |
|||
Particle Size | <= 500 µm | <= 500 µm | Grain Size |
Gouda Vuurvast ADHESIET 170 P Al Dry Air-Setting Refractory Mortar Description: Adhesiet 170 P Al is a phosphate bonded air setting mortar, supplied as a dry powder. Because of the special choice of raw materials this mortar is especially applied in aluminum meltin.. |
|||
Particle Size | <= 500 µm | <= 500 µm | Grain Size |
Gouda Vuurvast ADHESIET B Dry Air-Setting Refractory Mortar Description: Adhesiet B is a general purpose air setting mortar, supplied as a dry powder for use up to 1300°C.Remarks: Adhesiet mortars can be stored for an unlimited time if kept dry and cool. .. |
|||
Particle Size | 500 µm | 500 µm | Finer than |
Inhance Fluoro-Seal INHANCE® UH-1080 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Particle Size | <= 500 µm | <= 500 µm | ASTM D1921 |
Micropol HD Polyethylene powders for cleaning products Information provided by Micropol Limited |
|||
Particle Size | 500 - 5000 µm | 500 - 5000 µm | |
Minelco Chilcon Low grade FeSi Hard, wear resistant. Applications: Heavy aggregates, hard wearing floors |
|||
Particle Size | 500 - 2000 µm | 500 - 2000 µm | >90 |
Solvay Chemicals Ixper® 25M Magnesium Peroxide IXPER® 30M Magnesium Peroxide Granules are based on our commercial grade IXPER® 35M.EINECS Number: 215-627-7/CAS Number: 1335-26-8Information provided by Solvay |
|||
Particle Size | 500 - 900 µm | 500 - 900 µm | |
Shandong Dongyue Polymer DF-21A PTFE Presintered Resin Usage: The presintered resin is suitable for continuously extruding of all types, pushing and pressing PTFE rod, tube and special shape.Packing: PTFE is packed in double layer PVC bags inside and in.. |
|||
Particle Size | 500 - 700 µm | 500 - 700 µm | |
Shandong Dongyue Polymer DF-31A PTFE Pelletized Resin Usage: The resin is used to auto press molding and ram extrusion all kinds of rods, pipe etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTF.. |
|||
Particle Size | 500 - 1000 µm | 500 - 1000 µm | 50% Min; 540MA3C5E |
Solvay MIRAPOL® SURF-S 410 Surfactant Description: Granulated rinse aid polymer for use in automatic dish washing powders or tablets. 18% activeIdentification: BLEND OF ACRYLIC BASED POLYMER AND SODIUM TRIPOLYPHOSPHATE.Use level : 0.5 â.. |
|||
Particle Size | 500 µm | 500 µm | |
Daikin POLYFLON F-104 PTFE Fine Powder Processing Methods: Paste extrusion, calendering.Applications: Unsintered tape, sealing tape, low specific gravity tape, tape for wrapping flat cables, tubes.Information provided by Daikin Industrie.. |
|||
Particle Size | 500 µm | 500 µm | |
Daikin POLYFLON F-205 PTFE Fine Powder Processing Methods: Paste extrusion.Applications: Spaghetti tubes, small diameter tubes, fine electric wire smaller than AGW16.Information provided by Daikin Industries. |
|||
Particle Size | 500 µm | 500 µm | average; ISO 13320 |
3M Dyneon™ TF 2025Z PTFE Fine Powder Dyneon™ TF 2025 Z PTFE is an ideal grade for pipe liner applications in chemical plant construction due to high green strength.Product Features:High molecular weightFine powder grade for low to med.. |
|||
Particle Size | 500 µm | 500 µm | average; ISO 12086 |
3M Dyneon™ TF 2029Z PTFE Fine Powder Dyneon™ TF 2029 Z PTFE is an ideal grade for tapes with high mechanical strength, such as electrical tape for wrapped insulations or flat cables. Also ideal for yarn applications, including sewing .. |
|||
Particle Size | 500 µm | 500 µm | VW-10300P; D90 Particle sizes by sieve measurement |
Solvay Specialty Polymers Virantage® VW-10300 P, FP Polyethersulfone (PESU)
(Unverified Data**) Virantage® VW-10300 polyethersulfone (PESU) is a non-functionalized, high-temperature sulfone polymer powder. Two grades are offered: Virantage VW-10300P and Virantage VW-10300FP, providing two par.. |
|||
Particle Size | <= 500 µm | <= 500 µm | Grain Size |
Gouda Vuurvast ADHESIET 170 P Dry Air-Setting Refractory Mortar Description: Adhesiet 170 P is a phosphate bonded air setting mortar, supplied as a dry powder. Because of the special choice of raw materials this mortar is especially applied in aluminum melting a.. |