Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | >= 6.0 µm | >= 6.0 µm | 10% smaller than |
Nyco NYGLOS® M20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 6.0 µm | 6.0 µm | median; Microtrac |
Nyco NYGLOS® M3 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Particle Size | 6.0 µm | 6.0 µm | Median Grain Diameter |
Nabaltec APYRAL® 32 Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Particle Size | 6.0 µm | 6.0 µm | |
Poco Graphite CZR Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
Particle Size | 6.0 µm | 6.0 µm | Median Diameter |
Omya OMYACARB® 5 - FL Calcium Carbonate A beneficiated calcium carbonate with an intermediate and closely sized particle distribution.Applications: An ideal extender for plastics, rubber, coating, and caulks. Designed for use in unsaturat.. |
|||
Particle Size | 6.0 µm | 6.0 µm | Median Diameter |
Omya OMYACARB® 6 - PT Calcium Carbonate A dry ground calcium carbonate with intermediate and closely sized particle distribution.Applications: An ideal extender for plastics, rubber, coating, and caulks. Designed for use in unsaturated po.. |
|||
Particle Size | 6.0 - 10 µm | 6.0 - 10 µm | 10% finer than |
Potters Industries Sphericel® 60P18 Hollow Glass Spheres Description: This microsphere is strong with a density of 0.6g/cc, and has the added advantage of a very small particle size of only 18 micron (mean). Fused glass, hollow spheres used as an additive.. |
|||
Particle Size | <= 6.0 µm | <= 6.0 µm | <3% of particles are less than 20 microns |
Solvay Specialty Polymers Polymist® F-5A PTFE Powder Lubricant
(Unverified Data**) Polymist® powders are a family of white free-flowing polytetrafluoroethylene powders for use as additives in other materials to enhance processing or end-use performance characteristics. Polymist .. |
|||
Particle Size | 6.0 µm | 6.0 µm | 3rd Streak; Fineness of Grind |
Gwent Electronic Materials C2000107P3 Silver Ink Silver Ink C2000107P3 is designed as a termination for single layer PZT ceramics. After firing the film has good adhesion and solderability.The ink is in a ready to use form at a viscosity suitable.. |
|||
Particle Size | 6.0 µm | 6.0 µm | Crystal Size |
Momentive Performance Materials AC6069 Boron Nitride (BN) Powder GE Advanced Ceramics boron nitride (BN) powder grade AC6069 consists of single-crystal hexagonal particles with an average particle size of 9 µm. AC6069 has a relatively tight particle size distr.. |
|||
Particle Size | 6.0 - 9.0 µm | 6.0 - 9.0 µm | Mean |
Momentive Performance Materials HCPH Boron Nitride (BN) Powder GE Advanced Ceramics boron nitride (BN) powders of grades HCP, HCPH, HCPL, and AC6004 are generally single-crystal hexagonal platelets with very high purity. The mean particle sizes for these ultra-.. |
|||
Particle Size | <= 6.0 µm | <= 6.0 µm | 90% less than |
H.C. Starck Grade B Zirconium Diboride, ZrB2 Hot-pressed composites of excellent electrical conductivity, e.g., evaporation boats for continuous aluminum metallizingCrucible material for non-ferrous metalsCeramic shapes to be used in productio.. |
|||
Particle Size | 6.0 µm | 6.0 µm | |
Silberline Super Fine "N" Standard Series Super Fine N - is an ultra fine, high opacity, non-leafing aluminum pigment for solvent based industrial coatings. Due to the small particle size, this grade is well suited for imparting high opacit.. |
|||
Particle Size | 6.0 µm | 6.0 µm | Average Crystal Size - Thin Section Test |
CoorsTek AD-998 Alumina(nom. 99.8% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Particle Size | 6.0 µm | 6.0 µm | Average Crystal Size; THIN-SECTION |
CoorsTek ADD-96 96% Alumina |
|||
Particle Size | 6.0 µm | 6.0 µm | Average Crystal Size - Thin Section Test |
CoorsTek FG-995 Alumina (nom. 98.5% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Particle Size | 6.0 µm | 6.0 µm | Thin Section Crystal Size |
CoorsTek SC-DSG (SC-35) Graphite Loaded Sintered Silicon Carbide Thermal Shock Delta Tc = 600°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Particle Size | 6.0 µm | 6.0 µm | 30% less than 6 microns |
CIMBAR BARA 200 Barium Sulfate (BaSO4) BARA 200 is a natural barium sulfate. Cimbar's BARA 200 is designed to meet all the requirements of drilling grade barite. Bara meets or exceeds all API requirements. These properties make BARA 2.. |
|||
Particle Size | <= 6.0 µm | <= 6.0 µm | 50% |
BYK Cloisite® 15A Nanoclay Cloisite® 15A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr.. |
|||
Particle Size | <= 6.0 µm | <= 6.0 µm | 50% |
BYK Cloisite® 20A Nanoclay Cloisite® 20A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr.. |
|||
Particle Size | <= 6.0 µm | <= 6.0 µm | 50% |
BYK Cloisite® 25A Nanoclay Cloisite® 25A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr.. |
|||
Particle Size | <= 6.0 µm | <= 6.0 µm | 50% |
BYK Cloisite® 93A Nanoclay Cloisite® 93A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr.. |
|||
Particle Size | 6.0 - 12 µm | 6.0 - 12 µm | Mean particle size |
Carborundum CarboTherm™ CTH30 Boron Nitride Powder Boron Nitride powders have high thermal conductivity, low dielectric loss, and low thermal expansion. They are non-abrading to electronic components, lubricious, non-toxic, and retain their dielect.. |
|||
Particle Size | 6.0 - 9.0 µm | 6.0 - 9.0 µm | D(0.5) |
Akzo Nobel Expancel® 461 DU 20 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 6.0 - 9.0 µm | 6.0 - 9.0 µm | D(0.5) |
Akzo Nobel Expancel® 461 WU 20 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 6.0 - 10 µm | 6.0 - 10 µm | Mean particle size |
Carborundum CarboTherm™ CTF10 Boron Nitride Powder Boron Nitride powders have high thermal conductivity, low dielectric loss, and low thermal expansion. They are non-abrading to electronic components, lubricious, non-toxic, and retain their dielect.. |
|||
Particle Size | 6.0 - 12 µm | 6.0 - 12 µm | average |
Momentive Performance Materials PolarTherm® PT160 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic componen.. |
|||
Particle Size | <= 6.0 µm | <= 6.0 µm | 50% |
BYK Cloisite® 30B Nanoclay Cloisite® 30B is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.
Information provided by Southern Clay ProductsSouthern Clay P.. |
|||
Particle Size | <= 6.0 µm | <= 6.0 µm | 50% |
BYK Cloisite® Na+ Nanoclay Cloisite® Na+ is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr.. |