Polymer Property : Particle Size = 625 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 625 µm
625 µm
at a density of 2.10 g/cc
TIMCAL TIMREX® T150 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 625 µm
625 µm
at a density of 2.10 g/cc
TIMCAL TIMREX® T15-75 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 625 µm
625 µm
at a density of 2.10 g/cc
TIMCAL TIMREX® T200-2000 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 625 µm
625 µm
at a density of 2.10 g/cm<sup>3</sup>
TIMCAL TIMREX® T75 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 625 µm
625 µm
at a density of 2.10 g/cc
TIMCAL TIMREX® T800 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 625 µm
625 µm
at a density of 2.10 g/cc
TIMCAL TIMREX® T150-600 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..