Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 8.0 µm | 8.0 µm | median; Microtrac |
Nyco 400 WOLLASTOCOAT® Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Particle Size | 8.0 µm | 8.0 µm | median; Microtrac |
Nyco NYAD® 400 Wollastonite Chemically treated powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an .. |
|||
Particle Size | 8.0 µm | 8.0 µm | Median Grain Diameter |
Nabaltec APYRAL® 20X Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Particle Size | 8.0 µm | 8.0 µm | 50% finer than |
Potters Industries Sphericel® 110P8 Hollow Glass Spheres Description: Sphericel® 110P8 hollow glass spheres displace the same volume of resin as solid spheres of the same size, but are lighter. Using Sphericel® hollow glass spheres, plastics engineers c.. |
|||
Particle Size | <= 8.0 µm | <= 8.0 µm | Average; Internal Method |
Solvay Specialty Polymers Algoflon® L203 Polytetrafluoroethylene (PTFE)
(Unverified Data**) Algoflon® L203 is a white PTFE micropowder comprising loose agglomerates of sub-micron sized particles. It is recommended for use as an additive in high quality oils and greases to reduce coefficie.. |
|||
Particle Size | 8.0 - 11 µm | 8.0 - 11 µm | Mean particle size is 8 to 11 µm. Crystal size is 8 µm. %-325 mesh is 99.9%. |
Momentive Performance Materials HCPL Boron Nitride (BN) Powder All Grade HCP powders are high purity, fine (99%, -325 mesh), hexagonal Boron Nitride (BN). All exhibit the unique properties of BN in a form readily used in many advanced materials and processes. .. |
|||
Particle Size | 8.0 - 12 µm | 8.0 - 12 µm | 10% |
H.C. Starck Amperit® 519.059 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO) |
|||
Particle Size | 8.0 - 13 µm | 8.0 - 13 µm | 10% |
H.C. Starck Amperit® 544.059 Dense Coated Tungsten Carbide-Nickel 83-17 (WC-Ni) |
|||
Particle Size | 8.0 - 12 µm | 8.0 - 12 µm | 10% |
H.C. Starck Amperit® 558.059 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr) |
|||
Particle Size | 8.0 µm | 8.0 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade A Lanthanum Hexaboride, LaB6 Powder for cathodes. |
|||
Particle Size | <= 8.0 µm | <= 8.0 µm | 90% less than |
H.C. Starck Grade AT Yttrium Oxide Sintering additive for Si3N4 and ALNStabilizer for zirconias (PSZ) and insulating coatings (TBC`s)Catalyst carrierYttria stabilized zirconias electrolytes for solid oxide fuel cellsLuminescent mater.. |
|||
Particle Size | 8.0 µm | 8.0 µm | 50% of particles, (VEG Powder) |
Ferro EG 2928 Glaze and Sealant Glass Glass Type: Pb-Zn-B Typical Powder Form: VEG, MVG Typical Application: ZnO, Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective an.. |
|||
Particle Size | <= 8.0 µm | <= 8.0 µm | 3rd Streak; Fineness of Grind |
Gwent Electronic Materials C2031105D2 Palladium Ink Palladium Ink C2031105D2 is an ink formulated for screen printing for use on Fuel Cells. It is suitable for application onto Solid Oxide Fuel Cells.The ink has been made at a ready to use viscosity.. |
|||
Particle Size | <= 8.0 µm | <= 8.0 µm | 26% |
SGL Carbon Group CF 270 Graphite Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Particle Size | <= 8.0 µm | <= 8.0 µm | 28% |
SGL Carbon Group CF 5250 Carbon Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Particle Size | 8.0 µm | 8.0 µm | |
Silberline "A" Series A-2291FG A-2291FG is an ultra fine, high opacity, non-leafing aluminum pigment for solvent based general industrial coatings. Due to the small particle size, this grade is well suited for imparting high opac.. |
|||
Particle Size | 8.0 µm | 8.0 µm | Before Conversion |
Silberline Silvet® 330-20-E Silvet® E grades are economical aluminum pigments provided in pellet form for easy handling and incorporation. They are composed of 80% aluminum pigment and 20% polyolefin and are compatible with.. |
|||
Particle Size | 8.0 µm | 8.0 µm | |
Silberline SparkleBriteâ„¢ 320NL-PA SparkleBriteâ„¢ pigments are non-leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on cornflake geometry and produce strong metallic effects in solvent and wate.. |
|||
Particle Size | 8.0 - 12 µm | 8.0 - 12 µm | d90, Guaranteed |
TIMCAL TIMREX® C-LUB 304 Primary Synthetic Graphite Information provided by TIMCAL |
|||
Particle Size | 8.0 µm | 8.0 µm | d50 |
TIMCAL TIMREX® KS15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 8.0 µm | 8.0 µm | Thin Section Crystal Size |
CoorsTek SC-DSLP (SC-50) Liquid Phase Sintered Silicon Carbide Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Particle Size | 8.0 µm | 8.0 µm | Median |
Excalibar ExBar™ 400 Barite BaSO4 Powder ExBar™ industrial barytes products are manufactured from a high-quality natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, plastics, rubber, .. |
|||
Particle Size | 8.0 µm | 8.0 µm | Median |
Excalibar ExBar™ W 400 Barite BaSO4 Powder ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, .. |
|||
Particle Size | <= 8.0 µm | <= 8.0 µm | Max |
CIMBAR CIMBAR™ EX Barite Powder (BaSO4) CIMBAR barite products are made using only the highest quality white, natural barium sulfate ore. CIMBAR barites unique properties of fine grind, high specific gravity, low solubility and chemical .. |
|||
Particle Size | <= 8.0 µm | <= 8.0 µm | Max |
CIMBAR Miti-Wite B1 Chemically Purified White Barite (BaSO4) Miti-Wite barite products are produced using a proprietary chemical process to enhance the purity of the natural barium sulfate ore. Miti-Wite products are available in a variety of particle sizes .. |
|||
Particle Size | 8.0 - 12 µm | 8.0 - 12 µm | Average; ATO 40-41-0 (Coulter Counter) |
Arkema Group ORGASOL® 2002 EXD Nat 1 Polyamide 12, Food Contact Approved Information provided by Arkema Group |
|||
Particle Size | 8.0 - 25 µm | 8.0 - 25 µm | fiber diameter |
BCC Products BC 32 Fibrous Glass BC 32, microglass milled fibers will increase the mechanical strengths, such as impact strength, tensile strength, compressive strength, and flexural strength in plastic tooling compounds. They are .. |
|||
Particle Size | 8.0 µm | 8.0 µm | Average Diameter |
Potters Industries Conduct-O-Fil® SN08P40 Silver-coated Sub-10 micron Particles Conduct-O-Fil® conductive particles are engineered to meet a broad range of conductive and electro magnetic interference requirements. A variety of particle shapes offers the formulator additional .. |
|||
Particle Size | <= 8.0 µm | <= 8.0 µm | Main Break; Fineness of Grind |
Gwent Electronic Materials C2030304D2 Aluminum Ink C2030304D2 is designed as a screen printing ink for termination of Barium Titanate based PTC devices.This Ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen .. |
|||
Particle Size | 8.0 - 12 µm | 8.0 - 12 µm | 10% |
H.C. Starck Amperit® 547.002 Tungsten Carbide-Nickel 88-12 (WC-Ni) |