Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | >= 1000 m²/g | >= 1000 m²/g | BET |
Nanocyl NANOCYL™ NC1000 Single-Wall Isolated and Bundled Carbon Nanotubes - Research grade NANOCYL™ NC1000 series single-wall carbon nanotubes are produced via the catalytic carbon vapor deposition (CCVD) process. Nanotubes which exit the reactor are then purified to greater than 70% ca.. |
|||
Specific Surface Area | >= 1000 m²/g | >= 1000 m²/g | BET |
Nanocyl NANOCYL™ NC1100 Single-Wall Isolated and Bundled Carbon Nanotubes - Research grade NANOCYL™ NC1000 series single-wall carbon nanotubes are produced via the catalytic carbon vapor deposition (CCVD) process. Nanotubes which exit the reactor are then purified to greater than 70% ca.. |
|||
Specific Surface Area | 1000 m²/g | 1000 m²/g | Statistical thickness surface area; ASTM D 6556 |
Orion Engineered Carbons PRINTEX® XE 2B Conductive Carbon Black Specialty conductive carbon blackInformation provided by Orion Engineered Carbons. |
|||
Specific Surface Area | 1000 - 1100 m²/g | 1000 - 1100 m²/g | BET |
Beijing Evergrow Resources ACFP-100 Activated Carbon Fiber Powder Properties:High adsorption speed capacityGood efficiency towards pesticides and odorsPossible adaptation to condition of useHigh voluminal adsorption capacityRegenerableLow mineral contentApplicatio.. |
|||
Specific Surface Area | 1000 - 1100 m²/g | 1000 - 1100 m²/g | BET |
Beijing Evergrow Resources ACFP-20 Activated Carbon Fiber Powder Properties:High adsorption speed capacityGood efficiency towards pesticides and odorsPossible adaptation to condition of useHigh voluminal adsorption capacityRegenerableLow mineral contentApplicatio.. |
|||
Specific Surface Area | 1000 - 1100 m²/g | 1000 - 1100 m²/g | BET |
Beijing Evergrow Resources ACFP-200 Activated Carbon Fiber Powder Properties:High adsorption speed capacityGood efficiency towards pesticides and odorsPossible adaptation to condition of useHigh voluminal adsorption capacityRegenerableLow mineral contentApplicatio.. |
|||
Specific Surface Area | 1000 - 1100 m²/g | 1000 - 1100 m²/g | BET |
Beijing Evergrow Resources ACFP-400 Activated Carbon Fiber Powder Properties:High adsorption speed capacityGood efficiency towards pesticides and odorsPossible adaptation to condition of useHigh voluminal adsorption capacityRegenerableLow mineral contentApplicatio.. |
|||
Specific Surface Area | 1000 - 1100 m²/g | 1000 - 1100 m²/g | BET |
Beijing Evergrow Resources ACFP-60 Activated Carbon Fiber Powder Properties:High adsorption speed capacityGood efficiency towards pesticides and odorsPossible adaptation to condition of useHigh voluminal adsorption capacityRegenerableLow mineral contentApplicatio.. |