Physical Properties Metric English Comments
Specific Surface Area 50 - 70 m²/g
50 - 70 m²/g
BET
Nabaltec NABALOX® NO 201 Calcined Aluminum Oxide
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Specific Surface Area >= 50 m²/g
>= 50 m²/g
BET
NanoScale NanoActive® Cerium Oxide
NanoActive CeO2 is produced using proprietary processes to obtain high specific surface area, aggregated dry powder that can be dispersed in various carrier fluids to significantly reduce the partic..
Specific Surface Area 50 - 60 m²/g
50 - 60 m²/g
Zircar Zirconia ZYP-55 Zirconia Powder
Zircar Zirconia Powder Type ZYP is an ultra fine, highly reactive powder composed of yttria- stabilized zirconia. It is offered with two different surface areas; Type ZYP-55 has a surface area of 50..
Specific Surface Area 50 - 65 m²/g
50 - 65 m²/g
BET
Indium Corp. In(OH)3 Fine Indium Hydroxide
Indium Acetate is a white powder. Fine Powder Form: Primary particles range from 0.1 to 1.0 microns in size. they range in shape from spherical to elliptical to cylindrical. Agglomerates can be ..
Specific Surface Area 50 m²/g
50 m²/g
BET Nitrogen Surface Area; ASTM D3037
TIMCAL ENSACO™ 150G Conductive Carbon Black
ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can..
Specific Surface Area 50 - 60 m²/g
50 - 60 m²/g
Zircar Zirconia ZYP-55 Zirconia Powder
Zircar Zirconia Powder Type ZYP is an ultra fine, highly reactive powder composed of yttria- stabilized zirconia. It is offered with two different surface areas; Type ZYP-55 has a surface area of 50..
Specific Surface Area 50 - 500 m²/g
50 - 500 m²/g
American Elements Carbon Nanotubes
General DescriptionCarbon (C) Nanotubes, Single-Walled, Double Walled and Multi-Walled - Are black nano scale cylindrical tubes of graphitic carbon with numerous applications as the stiffest and str..
Specific Surface Area 50 m²/g
50 m²/g
BASF Heligoen® Blue 6989 F Color Additive
Description: Extremely reddish, e-phthalocyanine blue with high chroma and excellent flocculation resistanceChemical Structure: Cu-phthalocyanine, alpha-stabPhysical form: PowderSuitable for: Baking..