Physical Properties Metric English Comments
Specific Surface Area >= 80 m²/g
>= 80 m²/g
BET, Guaranteed
TIMCAL TIMREX® HSAG100 Primary Synthetic High Surface Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Specific Surface Area 80 m²/g
80 m²/g
BASF Heligoen® Blue L 6990 F Color Additive
Description: Highly transparent Phthalocyanine blue pigment with neutral flopChemical Structure: Cu-phthalocyanine, alpha-stabPhysical form: PowderSuitable for: Baking systems, Waterborn systems, Ac..
Specific Surface Area 80 m²/g
80 m²/g
BASF Sicotan® Yellow L 1916 Color Additive
Description: Transparent yellow iron oxideChemical Structure: Iron Oxide HydrateSuitable for: Waterborn systems, Acrylic-isocyanate systems, Acid curing system, Amine curing system and Airdrying sys..