Physical Properties | Metric | English | Comments |
---|---|---|---|
Antiblock Level | 6850 ppm | 6850 ppm | |
Bapolene® 152A Polyethylene Film Grade Bapolene 152A is a hexene linear low density polyethylene with a combination of superior impact strength and HSIT. Product is designed to exhibit performance similar to that of metallocene products... |