Physical Properties | Metric | English | Comments |
---|---|---|---|
Thermal Stress Crack Resistance | >= 1000 hour | >= 1000 hour | ASTM D 1693 |
Total Lacqtene® 2006 PBK 35 HDPE pipe, sheet
(discontinued **) LACQTENE® 2006 PBK 35 is a medium density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2006 PBK 35 may be used for pipe extrusion (micro-irriga.. |
|||
Thermal Stress Crack Resistance | >= 1000 hour | >= 1000 hour | ASTM D 1693 |
Total Lacqtene® 2006 TN 35 HDPE pipe coating
(discontinued **) LACQTENE® 2006 TN 35 is a medium density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2006 TN 35 may be used for pipe and sheet extrusion (flex.. |