Physical Properties | Metric | English | Comments |
---|---|---|---|
Fiber Count | 2.22 dtex | 2.00 denier | |
SGL Carbon Group PANOX® SA C063 EEA High performance oxidized textile fiber, Crimped staple fiber, For carbon/carbon and spinning PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX .. |
|||
Fiber Count | 2.22 dtex | 2.00 denier | |
SGL Carbon Group PANOX® SA C063 SSC High performance oxidized textile fiber, Crimped staple fiber, For felts and non-wovens PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX .. |
|||
Fiber Count | 2.22 dtex | 2.00 denier | |
SGL Carbon Group PANOX® SA T320 EEA High performance oxidized textile fiber, Continuous Tow with 320k filaments For carbon/carbon and spinning. PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not b.. |
|||
Fiber Count | 2.22 dtex | 2.00 denier | |
SGL Carbon Group PANOX® SM C063 EEA Oxidized Textile Fiber, Crimped staple fiber, For carbon/carbon and spinning PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX .. |
|||
Fiber Count | 2.22 dtex | 2.00 denier | |
SGL Carbon Group PANOX® SM C063 SSC Oxidized Textile Fiber, Crimped staple fiber, For felts and non-wovens PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX .. |
|||
Fiber Count | 2.22 dtex | 2.00 denier | |
SGL Carbon Group PANOX® SM C076 SSC Oxidized Textile Fiber, Crimped staple fiber, For felts and non-wovens PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX .. |
|||
Fiber Count | 2.22 dtex | 2.00 denier | |
SGL Carbon Group PANOX® SM T320 EEA Oxidized Textile Fiber, Continuous Tow with 320k filaments, For carbon/carbon and spinning PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX .. |