Polymer Property : Fiber Count = 8940 dtex Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Fiber Count 8940 dtex
8050 denier
Warp yarn; HM Aramid
Hexcel® HexForce™ KA090 Aramid and High Performance Fabrics
Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid..