Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00200 cm/cm | 0.00200 in/in | ASTM D955 |
Niche Polymer PA6GF43N Nylon 6, 43% Glass Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00200 cm/cm | 0.00200 in/in | ASTM D955 |
Niche Polymer PA6GF50BK Nylon 6, 50% Glass Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00200 - 0.0220 cm/cm | 0.00200 - 0.0220 in/in | Average value: 0.0118 cm/cm Grade Count:101 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00600 cm/cm | 0.00200 - 0.00600 in/in | Average value: 0.00404 cm/cm Grade Count:12 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00300 cm/cm | 0.00200 - 0.00300 in/in | Average value: 0.00267 cm/cm Grade Count:3 |
Overview of materials for PCT, 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00600 cm/cm | 0.00200 - 0.00600 in/in | Average value: 0.00359 cm/cm Grade Count:17 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00700 cm/cm | 0.00200 - 0.00700 in/in | Average value: 0.00500 cm/cm Grade Count:3 |
Overview of materials for Polyarylsulfone (PAS), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyarylsulfone; Molded/Extruded". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0114 cm/cm | 0.00200 - 0.0114 in/in | Average value: 0.00556 cm/cm Grade Count:81 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0100 cm/cm | 0.00200 - 0.0100 in/in | Average value: 0.00671 cm/cm Grade Count:7 |
Overview of materials for Polyphenylene Ether, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, PTFE Filled". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00552 cm/cm Grade Count:106 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00530 cm/cm Grade Count:54 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00420 cm/cm Grade Count:10 |
Overview of materials for Acrylic, High Flow, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, High Flow, Molded". Each property range of values reported is minimum and maximum values of app.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0400 cm/cm | 0.00200 - 0.0400 in/in | Average value: 0.0108 cm/cm Grade Count:35 |
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00200 cm/cm @Temperature 80.0 - 80.0 °C |
0.00200 - 0.00200 in/in @Temperature 176 - 176 °F |
Average value: 0.00200 cm/cm Grade Count:6 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00600 cm/cm | 0.00200 - 0.00600 in/in | Average value: 0.00400 cm/cm Grade Count:10 |
Overview of materials for Nylon 11 with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are includ.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0150 cm/cm | 0.00200 - 0.0150 in/in | Average value: 0.00602 cm/cm Grade Count:69 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0213 cm/cm | 0.00200 - 0.0213 in/in | Average value: 0.0139 cm/cm Grade Count:39 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00600 cm/cm | 0.00200 - 0.00600 in/in | Average value: 0.00400 cm/cm Grade Count:19 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0160 cm/cm | 0.00200 - 0.0160 in/in | Average value: 0.00520 cm/cm Grade Count:7 |
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00504 cm/cm Grade Count:104 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00900 cm/cm | 0.00200 - 0.00900 in/in | Average value: 0.00491 cm/cm Grade Count:7 |
Overview of materials for Polypropylene with Glass Fiber + Bead Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00400 cm/cm | 0.00200 - 0.00400 in/in | ASTM D955 |
Bhansali Engineering Abstron IM17SHG PMMA- ABS Alloy High GlossInformation provided by Bhansali |